MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Low-leaded brass tube, UNS C33000, H58 Temper
Categories: Metal; Nonferrous Metal; Copper Alloy; Brass

Material Notes: Fair to excellent corrosion resistance. Combines good machinability and excellent cold workability. Fabricated by forming and bending, machining, piercing and punching.

Applications: pump and power cylinders and liners, ammunition primers, plumbing accessories.

Test specimen: tubing - 25mm OD x 1.65mm wall thickness.

Key Words: CDA 330
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.50 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 70
Hardness, Rockwell F 100
Hardness, Rockwell 30T 66
Tensile Strength, Ultimate 450 MPa
Tensile Strength, Yield 345 MPa
@Strain 0.5 %
Elongation at Break 32 %In 50 mm
Modulus of Elasticity 105 GPa
Poissons Ratio 0.346
Machinability 60 %UNS C36000 (free-cutting brass) = 100%
Shear Modulus 39.0 GPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000660 ohm-cm
@Temperature 20.0 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 20.2 µm/m-°C
@Temperature 20.0 - 300 °C
Specific Heat Capacity 0.380 J/g-°C
Thermal Conductivity 115 W/m-K
@Temperature 20.0 °C
Melting Point 905 - 940 °C
Solidus 905 °C
Liquidus 940 °C
Annealing Point 800 - 1200 °F
 
Processing PropertiesOriginal ValueComments
Annealing Temperature 425 - 650 °C
Recrystallization Temperature 290 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 65 - 68 %
Iron, Fe <= 0.070 %
Lead, Pb 0.20 - 0.80 %
Other, total <= 0.50 %
Zinc, Zn 33.5 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Forging Brass, UNS C37700
Medium-leaded brass, UNS C35000, H03 Temper flat products
High-leaded brass, UNS C34200
Low-leaded brass tube, UNS C33000
Low-leaded brass, UNS C33500

MC33000b4 / 11170

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.