MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Kingfa NH-627 Flame Retardant ABS
Categories: Polymer; Thermoplastic; ABS Polymer; Acrylonitrile Butadiene Styrene (ABS), Unreinforced, Flame Retardant

Material Notes:
    Features:
  • UL 94 V-2 @ 1.6mm
  • Halogen-free flame retardant
  • High flow

    Applications:
  • OA device
  • Digital camera
  • Vidicon

Information Provided by Kingfa Sci. & Tech. Co., Ltd.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.06 g/cc
@Temperature 23.0 °C
ASTM D792
Linear Mold Shrinkage 0.0040 - 0.0070 cm/cm
@Temperature 23.0 °C
ASTM D955
Melt Flow 5.0 g/10 min
@Load 5.00 kg,
Temperature 200 °C
ASTM D1238
 55 g/10 min
@Load 10.0 kg,
Temperature 220 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 102ASTM D785
Tensile Strength at Break 45.0 MPa50mm/min; ASTM D638
Elongation at Break 10 %50mm/min; ASTM D638
Flexural Strength 70.0 MPa2mm/min; ASTM D790
Flexural Modulus 2500 MPa2mm/min; ASTM D790
Izod Impact, Notched 125 J/m
@Thickness 6.40 mm,
Temperature 23.0 °C
ASTM D256
 145 J/m
@Thickness 3.20 mm,
Temperature 23.0 °C
ASTM D256
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+14 ohm-cmASTM D257
Dielectric Strength 22.0 kV/mmASTM D149
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 0.46 MPa (66 psi) 80.0 °C
@Thickness 6.40 mm
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 72.0 °C
@Thickness 6.40 mm
ASTM D648
Vicat Softening Point 81.0 °C
@Load 5.00 kg
50°C/hr; ASTM D1525
 90.0 °C
@Load 1.00 kg
120°C/hr; ASTM D1525
Flammability, UL94 V-2
@Thickness 1.60 mm
 V-2
@Thickness 0.800 mm
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 250 °C
Rear Barrel Temperature 180 - 200 °CStart Point: 190°C
Middle Barrel Temperature 190 - 210 °CStart Point: 200°C
Front Barrel Temperature 195 - 220 °CStart Point: 210°C
Melt Temperature 200 - 230 °CStart Point: 215°C
Mold Temperature 30.0 - 60.0 °CStart Point: 50°C
Drying Temperature 70.0 °C
@Time 7200 sec
Pre-dry
Back Pressure 0.000 - 1.00 MPa
 
Descriptive Properties
Injection SpeedSlow to Moderate

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Kingfa JH960 6300 Non-halogenated Flame Retardant PC/ABS Alloy
INEOS Styrolution Terluran® GP-22 ABS

PKINGF111 / 104370

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.