MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC VALOX™ FR Resin ENH4550 Polybutylene Terephthalate (PBT) (Americas)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: VALOX ENH4550 is a 25% glass reinforced, non-chlorinated/brominated flame retardant Polybutylene Terephthalate (PBT) injection moldable grade with excellent chemical resistance. It has a UL94V0@0.30mm and 5VA@2.0mm flame rating. This is a good candidate for a variety of applications needing a sustainable FR PBT solution.

Features: Chemical Resistance,Flame Retardant,Non-Chlorinated,Non-Brominated,ECO Compliant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.52 g/ccASTM D792
Density 1.52 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.0600 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.23 %ISO 62-1
Viscosity 210000 cPmelt; ISO 11443
 18 cP
@Load 5.00 kg,
Temperature 250 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0010 - 0.0050 cm/cmSABIC method
 0.0010 - 0.0050 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0060 - 0.012 cm/cmSABIC method
 0.0050 - 0.011 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 25 g/10 min
@Load 5.00 kg,
Temperature 250 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 112 MPa5 mm/min; ISO 527
 115 MPa5 mm/min; ASTM D638
Tensile Strength, Yield 112 MPa5 mm/min; ISO 527
 115 MPa5 mm/min; ASTM D638
Elongation at Break 2.0 %5 mm/min; ASTM D638
 2.0 %5 mm/min; ISO 527
Elongation at Yield 2.0 %5 mm/min; ASTM D638
 2.0 %5 mm/min; ISO 527
Tensile Modulus 10300 MPa5 mm/min; ASTM D638
 10400 MPa1 mm/min; ISO 527
Flexural Strength 165 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 175 MPayield, 2 mm/min; ISO 178
Flexural Modulus 8800 MPa1.3 mm/min, 50 mm span; ASTM D790
 9200 MPa2 mm/min; ISO 178
Flexural Strain at Break 2.0 %2 mm/min; ISO 178
Izod Impact Notched 70.0 JASTM D256
 65.0 J
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched 550 J/mASTM D4812
 525 J/m
@Temperature -30.0 °C
ASTM D4812
Izod Impact, Notched (ISO) 8.00 kJ/m²80*10*4; ISO 180/1A
 8.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²80*10*4; ISO 180/1U
 35.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 45.0 kJ/m²ISO 179/2C
 40.0 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
Charpy Impact, Notched 5.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 8.00 kJ/m²ISO 179/2C
 8.00 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
Dart Drop, Total Energy 6.00 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmASTM D257
 1.00e+15 ohm-cmIEC 60093
Dielectric Strength 20.0 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
 21.0 kV/mm
@Thickness 3.20 mm
in air; ASTM D149
Comparative Tracking Index 300 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 22.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E831
 22.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 24.3 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 28.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 63.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 71.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 77.0 µm/m-°C
@Temperature -40.0 - 150 °C
ASTM E831
 91.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 220 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 220 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 207 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 205 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 205 °CRate B/50; ASTM D1525
 207 °CRate B/50; ISO 306
 208 °CRate B/120; ISO 306
 215 °CRate A/50; ASTM D1525
 220 °CRate A/50; ISO 306
Glow Wire Ignition Temperature 775 °C
@Thickness 3.00 mm
IEC 60695-2-13
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 230 - 255 °C
Zone 2 235 - 250 °C
Zone 3 240 - 260 °C
Melt Temperature 245 - 260 °CInjection Molding
Mold Temperature 40.0 - 100 °C
Drying Temperature 110 - 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Precipitation Temperature 40.0 - 60.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82778 / 290725

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.