MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
EMS-Grivory Grilamid® TR 90 UV PAMACM12
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Nylon 12 (PA12)

Material Notes: Product description: Grilamid TR 90 UV natural is a high purity transparent thermoplastic polyamide, based on aliphatic and cycloaliphatic monomers. Grilamid 90 UV natural offers outstanding properties such as:
  • Transparency and maximum possible weathering stability
  • Unlimited colourability
  • Stress crack resistance
  • Toughness and stiffness
  • Good chemical resistance
  • High flexural fatigue strength
Grilamid TR 90 natural is especially suited for injection moulded outdoor applications in the application fields of:
  • Optics
  • Automotive
  • Mechanical engineering
  • Safety technology
  • Electro / Electronics

Information provided by EMS Grivory.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.00 g/ccDry; ISO 1183
Water Absorption 3.0 %Sim. to ISO 62
Moisture Absorption 1.50 %Sim. to ISO 62
Linear Mold Shrinkage, Flow 0.0070 cm/cmISO 294-4, 2577
Linear Mold Shrinkage, Transverse 0.0080 cm/cmISO 294-4, 2577
 
Mechanical PropertiesOriginal ValueComments
Tensile Modulus 1600 MPaDry; ISO 527-1/-2
 1600 MPaConditioned; ISO 527-1/-2
Charpy Impact Unnotched NB
@Temperature 23.0 °C
Conditioned; ISO 179/1eU
 NB
@Temperature -30.0 °C
Conditioned; ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²
@Temperature -30.0 °C
Conditioned; ISO 179/1eA
 10.0 kJ/m²
@Temperature 23.0 °C
Conditioned; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+11 ohm-cmConditioned; IEC 60093
Surface Resistance 1.00e+11 ohmIEC 60093
Dielectric Strength 31.0 kV/mmConditioned; IEC 60243-1
Comparative Tracking Index 600 VConditioned; IEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 90.0 µm/m-°CISO 11359-1/-2
CTE, linear, Transverse to Flow 90.0 µm/m-°CISO 11359-1/-2
Deflection Temperature at 0.46 MPa (66 psi) 135 °CISO 75-1/-2
Deflection Temperature at 1.8 MPa (264 psi) 115 °CISO 75-1/-2
Glass Transition Temp, Tg 155 °C10°C/min; ISO 11357-1/-2
Flammability, UL94 HBIEC 60695-11-10
 
Optical PropertiesOriginal ValueComments
Transmission, Visible 90 %transparent; thickness not quantified
 
Descriptive Properties
AutomotiveAutomotive electr. and electronics, lighting
 Cooling and climate control
 Exterior
 Fuel systems
 Interior
 Powertrain and Chassis
Electricals & ElectronicsElectrical equipment
 Lighting
FormGranules
Industry & Consumer goodsHydraulics & Pneumatics
 Mechanical Engineering
 Sports & Leisure
 Tools & Accessories
ProcessingInjection Molding
 Other Extrusion
Special CharacteristicsImproved UV resistance (outdoor use)
 Light stabilized or stable to light
 Transparent

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
EMS-Grivory Grilamid® TR 90 PAMACM12
EMS-Grivory Grilamid® TR 90 LXS PAMACM12
EMS-Grivory Grilamid® TR 30 nat PA*
EMS-Grivory Grilamid® TR 90 NZ PAMACM12-I
EMS-Grivory Grilamid® TR 90 NZZ nat PAMACM12-I

PGRH106 / 156815

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.