MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Mar-Bal MB1000-25 Thermoset Polyester Composite Molding Compound
Categories: Polymer; Thermoset; Polyester, TS; Thermoset Polyester Glass Filled BMC

Material Notes: A general purpose material that is easily customized. Designed for Powder Coating and Electrostatic painting.

Mar-Bal standard grades can be injection, compression and transfer molded.

Information provided by Mar-Bal, Inc.

Vendors: Mar-Bal is the leading integrated compounder and molder of BMC Thermoset composite products and value added finishing services. Call 440-543-7526 or visit Mar-Bal.com

Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.70 - 1.90 g/ccASTM D792
Bulk Factor 3.0ASTM D1895
Filler Content 25 %Glass
Water Absorption 0.13 %
@Time 86400 sec
ASTM D570
Linear Mold Shrinkage 0.00050 - 0.0020 in/inASTM D955
 
Mechanical PropertiesOriginal ValueComments
Hardness, Barcol 45 - 55ASTM D2583
Tensile Strength 8.00 - 10.0 ksiASTM D638
Flexural Strength 19.0 - 22.0 ksiASTM D790
Flexural Modulus 1600 - 1700 ksiASTM D790
Compressive Strength 20.0 - 24.0 ksiASTM D695
Shear Strength 7.00 - 9.00 ksiASTM D732
Izod Impact, Notched 7.00 - 10.0 ft-lb/inASTM D256
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 355 V/milASTM D149
Arc Resistance >= 140 secASTM D495
Track Resistance 3000 secInclined-Plane Tracking; ASTM D2303
 
Thermal PropertiesOriginal ValueComments
Deflection Temperature at 1.8 MPa (264 psi) >= 500 °FASTM D648
Flammability, UL94 HB
 
Descriptive Properties
Listed File E80533No

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Mar-Bal AltraSet MB2000-25 Thermoset Polyester - Flame and Tracking Resistant Grade
Mar-Bal MB2000-15 Thermoset Polyester Composite Molding Compound
Mar-Bal AltraSet MB5500 Thermoset Polyester - Superior Heat Resistance Grade
Mar-Bal AltraSet MB4000 Thermoset Polyester - Superior Tracking Resistance Grade
Mar-Bal AltraSet MB3000-20NY Thermoset Polyester - Non-Yellowing Grade

PMARB904 / 149942

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.