MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
ExxonMobil LDPE LD 200.48 Low Density Polyethylene Resin
Categories: Polymer; Thermoplastic; Polyethylene (PE); Low Density (LDPE)

Material Notes: Product Description: LD 200.48 is a general purpose LDPE extrusion coating grade, designed for flexible packaging applications. It offers – Low neck-in – Very good adhesion – Excellent heat sealability (ie high seal speeds and/or low heat seal temperatures mostly required in high speed form-fill-and-seal applications.

Availability: Latin America, North America and South America

Additive:

  • Antiblock: No
  • Slip: No
  • Thermal Stabilizer: Yes
Applications:
  • Coextrusion Coating
  • Extrusion Coating
  • Extrusion Lamination
  • Food packaging
  • Low Neck In, Low Line Speed Coatings
  • Photographic Paper

Information provided by ExxonMobil

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.915 g/ccExxonMobil method
Melt Flow 7.5 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Neck In 1.30 in328 ft/min, Constant output at 35 rpm; ExxonMobil Method
 1.40 in164 ft/min, Constant output at 35 rpm; ExxonMobil Method
Drawdown 1.83 m/sConstant output at 35 rpm; ExxonMobil Method
 
Thermal PropertiesOriginal ValueComments
Melting Point <= 219 °FPeak Melting Point; ExxonMobil method
Vicat Softening Point 185 °FASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Huntsman PE1059 Film Extrusion Polyethylene
Huntsman PE5050 Extrusion Coating Polyethylene
ExxonMobil LDPE LGA 105 Low Density Polyethylene Resin
Westlake EC472 Low Density Polyethylene
LyondellBasell Lupolen 2420K Low Density Polyethylene (LDPE), Film Grade

PEX99218 / 175454

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.