MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Dow Buna® cis 132 High-cis polybutadiene rubber (nickel catalyzed) for tires and rubber articles
Categories: Polymer

Material Notes: Buna® cis 132 - Schkopau is a stereospecific polybutadiene with high cis-1,4 content. It is manufactured by a solution process using an organo-metallic catalyst which produces a consistent light colored polymer with low ash content. It contains a non-staining stabilizer. Buna® cis 132 is widely used in the tire industry but also in the manufacture of conveyor belts and other rubber articles which are exposed to high stress. It offers good abrasion resistance, high resilience, low hysteresis, and low glass transition point which results in better low temperature performance.

Buna® cis 132 offers excellent processability and may be blended with natural rubber and styrene butadiene (SBR), isoprene (IR), nitrile (NBR), or polychloroprene (CR) synthetic rubbers. The non-staining stabilizer allows manufacture of colored rubber articles also when compounded with selected thermoplastics. It is supplied in bales weighing 25 kg. Bales are wrapped in 50 micron PE film.

Information provided by Dow

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Viscosity Measurement 3.1[min]; ts1; ASTM D5289
 6.9[min]; tc(50); ASTM D5289
 10.5[min]; tc(90); ASTM D5289
 16[dNm]; MH; ASTM D5289
 2.6
@Temperature 160 °C
[dNm]; ML; ASTM D5289
Mooney Viscosity 45
@Temperature 100 °C
[MU]; ML 1+4; ASTM D1646
Ash 0.050 %ASTM D5667
Collected Volatile Condensable Material 0.25 %ASTM D5668
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength, Ultimate 17.5 MPaCure: 35 min at 145°C; ASTM D412
Tensile Stress at Strain 9.00 MPa
@Strain 300 %
ASTM D412
Elongation at Break 510 %ASTM D412
 
Processing PropertiesOriginal ValueComments
Shelf Life >= 12.0 Month
 
Descriptive Properties
Accelerator (TBBS) wt%0.9ASTM D3189
Carbon Black wt%60ASTM D3189; IRB 7
Cis-1,4 Content %95Supplier Method (FTIR)
Stearic Acid wt%2ASTM D3189
Sulfur content, %1.5ASTM D3189
Zinc Oxide wt%3ASTM D3189

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Nitrile Rubber (NBR, Acrylonitrile-Butadiene Rubber)
Process Technologies Inc BUNA-N Sanitary Gasket
Trinseo BUNA™ cis 132 Schkopau High-cis Polybutadiene Rubber (PBR)
ATG s.r.l. BR Polybutadiene Rubber
Polybutadiene Rubber (BR)

PDOW1016 / 30220

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.