MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
KLJ Group Kanatol 8 S Plasticizer
Categories: Fluid

Material Notes: Properties: DOS is almost colourless and oily liquid, free of foreign materials.

Application: Dioctyl Sebacate is a plasticizer for PVC, and its copolymers, nitrocelluloses, styrene resins and synthetic rubbers where low temperature performance is required. The end applications include anti-frosting cable and PVC linoleum.

Chemical Name: Di (2-Ethylhexyl) Sebacate

Molecular Formula: C 26 H50 O 4

Molecular Structure: (CH2 ) 8 (COOC 8 H 12 )2

CAS Number: 122-62-3, 131170-17-7 , 28986-40-5

EINECS NO.: 204-558-8

Information provided by KLJ Group

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.910 - 0.916 g/cc
@Temperature 27.0 °C
ASTM D1045-08
Viscosity 58 - 64 cPKLJ TM-P-13-97
Molecular Weight 426 g/mol
 
Thermal PropertiesOriginal ValueComments
Boiling Point 248 °C
@Pressure 0.000667 MPa
Flash Point >= 215 °C
 
Optical PropertiesOriginal ValueComments
Refractive Index 1.447 - 1.453
@Temperature 27.0 °C
ASTM D1045-08
 
Processing PropertiesOriginal ValueComments
Moisture Content <= 0.10 %ASTM D1045-08
Shelf Life 24.0 Month
 
Descriptive Properties
Acidity after heat treatment<0.03%180°C for 2 hrs, ISI-9591-03
Acidity as Acid<0.02%ASTM D1045-08
AppearanceWater White Clear Liquid
Color<40Hazen, ASTM D1045-08
Content>99.5%Ester Content, ASTM D1045-08
 >99.5%Plasticizing Ester by GLC, KLJ TM-P-12-98
 260-266 mg KOH/gmEster Value, ASTM D1045-08
Volatile Loss<0.2%130°C for 3 hrs, KLJ TM-P-11-92

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PKLJ171 / 284192

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.