MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nouryon Armostat 300 Tallow-bis(2-hydroxyethyl) amine
Categories: Other Engineering Material

Material Notes: Semi-permanent, animal-based antistat providing sustained antistatic properties and is especially effective in film applications.

Applications: Armostat 300 is an internal antistatic additive that can be used in various polymers such as PE, LDPE and PP. Armostat 300 gives sustained antistatic action and is especially effective in film applications also due to its relative fast migration. Armostat 300 is at ambient temperature a paste. When heated at 40-45°C the product can be dosed as a liquid directly into the polymer by using a single or twin-screw extruder. Pigment or color concentrates should be mixed with the antistatic agent prior to extruding. Premixing ensures uniform distribution of Armostat 300 in the resin while Armostat 300 acts as a dispersion aid to the pigment color concentrate.

CAS number: 61791-44-4

EINECS/ELINCS No.: 263-177-5

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.890 g/cc
Viscosity 75 cP
Vapor Pressure <= 0.000100 bar
 
Thermal PropertiesOriginal ValueComments
Melting Point 32.0 °C
Flash Point 201 °CCleveland open cup
Ignition Temperature 285 °CAutoignition
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 0.20 %
 
Descriptive Properties
AppearanceLiquid to paste
Color= 200 Pt-Co
Content=97.0 %tert-Amine
Equivalent weight340-360 g/eq

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY262 / 285785

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.