Description: BRALEN+ FA 03-01 is a film grade of low density polyethylene with good processability, flexibility, toughness and good tear strength. This grade is additives free. Applications: BRALEN+ FA 03-01 is designed for production of heavy duty and shrink films. It is well suited for blow molding of various containers, bottles, pipes, sheets and profiles extrusion and for injection molding. Recommended film thickness is 0.07 to 0.22 mm. (1) Density has been measured on pressed mould specimen according to internal method. (2) Film properties tested using 50 µm thick blown film extruded at melt temperature of 200 °C and blow up ratio 2.5:1. (3) Typical properties measured on standard injection molded test specimen according to ISO 294-1. Information provided by Molgroup Chemicals |