MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC ULTEM™ Resin AUT200G4 Polyetherimide (PEI)
Categories: Polymer; Thermoplastic; Polyetherimide (PEI)

Material Notes: 20% Glass fiber filled, enhanced flow Polyetherimide (Tg 217C).

Features: High Stiffness,Hydrolytic Stability,Chemical Resistance,Easy Flow,Low Smoke and Toxicity,Good Mechanicals in Broad Temperature Range,Low Creep Sensitivity,Low Shrinkage,Good metal adhesion,Amorphous,High Strength,General Purpose,High Heat Resistance,Good dimensional stability,Flame Retardant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.42 g/ccASTM D792
Density 1.42 g/ccISO 1183
Moisture Absorption 0.0200 %Injection Molding
 0.550 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 1.0 %ISO 62-1
Viscosity 10 cP
@Load 5.00 kg,
Temperature 360 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0030 - 0.0050 cm/cmSABIC method
Melt Flow 8.4 g/10 min
@Load 6.60 kg,
Temperature 337 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 150 MPaH358/30; ISO 2039-1
Tensile Strength at Break 139 MPa5 mm/min; ASTM D638
 140 MPa5 mm/min; ISO 527
Elongation at Break 2.0 %5 mm/min; ISO 527
 4.0 %5 mm/min; ASTM D638
Tensile Modulus 6800 MPa1 mm/min; ISO 527
 6890 MPa5 mm/min; ASTM D638
Flexural Strength 210 MPabreak, 2mm/min; ISO 178
 227 MPabrk, 2.6 mm/min, 100 mm span; ASTM D790
Flexural Modulus 6500 MPa2 mm/min; ISO 178
 6890 MPa2.6 mm/min, 100 mm span; ASTM D790
Izod Impact Notched 64.0 JASTM D256
 453 J
@Thickness 3.20 mm
reverse notched; ASTM D256
Izod Impact, Unnotched 475 J/mASTM D4812
Izod Impact, Unnotched (ISO) 30.0 kJ/m²80*10*4; ISO 180/1U
 30.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 35.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 35.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 9.00 kJ/m²ISO 179/2C
Taber Abrasion, mg/1000 Cycles 17CS-17, 1 kg; SABIC method
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity 1.00e+15 ohm-cmIEC 60093
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 3.0
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 50.0 - 60.0 Hz
IEC 60250
Dielectric Strength 16.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 26.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
 34.0 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
Dissipation Factor 0.00080
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.0025
@Frequency 1e+6 Hz
IEC 60250
Comparative Tracking Index 150 VIEC 60112
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 21.0 µm/m-°C
@Temperature -20.0 - 150 °C
ISO 11359-2
CTE, linear, Transverse to Flow 49.0 µm/m-°C
@Temperature -20.0 - 150 °C
ISO 11359-2
Thermal Conductivity 0.280 W/m-KISO 8302
Deflection Temperature at 0.46 MPa (66 psi) 210 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 210 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 205 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 211 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 212 °CRate B/50; ISO 306
 218 °CRate B/120; ISO 306
 223 °CRate A/50; ISO 306
 225 °CRate B/50; ASTM D1525
UL RTI, Mechanical with Impact 170 °CUL 746B
UL RTI, Mechanical without Impact 170 °CUL 746B
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 360 - 410 °C
Zone 2 360 - 410 °C
Zone 3 370 - 420 °C
Melt Temperature 370 - 410 °CInjection Molding
Mold Temperature 140 - 180 °C
Drying Temperature 150 °CInjection Molding
Dry Time 4.00 - 6.00 hourInjection Molding
Precipitation Temperature 80.0 - 120 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82667 / 290614

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.