Description: - MAGRAM absorber that utilizes a thermoplastics elastomer binder to provide a good balance of electrical and mechanical properties.
- Designed for surface current attenuation over a wide range of frequencies, particularly above 3GHz.
- Ideally suited as a near-field absorber/suppressor in electronic enclosures or as a wave guide termination.
- Can be injection molded in a wide variety of shapes and sizes or extruded into sheet form.
- Halogen free, RoHS and REACH compliant.
Information provided by Hexcel Corporation. |