Standard Applications: RHODACALĀ® SS-40/A has excellent handling characteristics and is especially suitable for the manufacture of liquid detergents allowing formulation over a wide range of concentrations and viscosities. Chemical Name: SODIUM ALKYL BENZENE SULFONATE CAS No: 68081-81-2 Information provided by Solvay |