System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
Titanium Copper (TiCuR1), EH Temper
Categories:
Metal
;
Nonferrous Metal
;
Copper Alloy
;
Wrought Copper
Material Notes:
Composition is 99.5% Cu+Ti minimum. Product forms include sheet and strip. Used in connectors, switches, relays, and other electronic devices. Information taken from Nippon Mining and Metals Co. literature.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
8.70
g/cc
Mechanical Properties
Original Value
Comments
Hardness, Vickers
300 - 350
Tensile Strength, Ultimate
930
MPa
Elongation at Break
>= 5.0 %
Modulus of Elasticity
127
GPa
Electrical Properties
Original Value
Comments
Electrical Resistivity
0.0000133
ohm-cm
Thermal Properties
Original Value
Comments
CTE, linear
18.6
µm/m-°C
@Temperature 30.0 - 450 °C
Melting Point
1040
-
1070
°C
Solidus
1040
°C
Liquidus
1070
°C
Component Elements Properties
Original Value
Comments
Copper, Cu
96.4 %
Titanium, Ti
2.9 - 3.4 %
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Titanium Copper (TiCuR1), 1/4 Hard Temper
Goodfellow Copper 90/Titanium 10 Alloy
Beryllium Copper, UNS C17300, TH04 Temper wire, 2-9.5 mm
Goodfellow Copper 70/Titanium 30 Alloy
Overview of materials for Copper Alloy
MCUTi1 / 11997
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.