MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Green Dot Terratek® BD3002 (RD022615-2) Biodegradable polymers
Categories: Polymer; Renewable/Recycled Polymer

Material Notes: Product Description: Terratek® BD3002 (RD022615-2) Blown Film sample. Terratek® BD3002 (RD022615-2) is a proprietary blend of natural and synthetic biodegradable polymers. The resin is made with ingredients which pass industry standards for composting. This formula was developed for blown and cast film applications.

Information provided by Green Dot Bioplastics

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Water Vapor Transmission 16.1 g/100 in²/day23°C, 85% RH
Oxygen Transmission Rate 49.6 cc/100 in²/day23°C, 0% RH
Thickness 2.00 mil
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 578 %ASTM D882-12
Film Elongation at Break, TD 592 %ASTM D882-12
Modulus of Elasticity 1640 ksiTD; ASTM D882-12
 6170 ksiMD; ASTM D882-12
Film Tensile Strength at Break, MD 1920 psiASTM D882-12
Film Tensile Strength at Break, TD 1500 psiASTM D882-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 300 - 340 °Fbarrel temperatures
Melt Temperature <= 400 °F

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PGREEND5015 / 312286

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.