MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Pyrotek Thermollite Insulating Refractory Shapes for Molten Aluminum
Categories: Ceramic

Material Notes: Thermollite has been specifically developed for direct contact with molten aluminum and its various alloys. Thermollite provides the specific advantage of reducing heat loss in melt transfer applications involving a low rate of metal flow.

Applications

  • Continuous Casting Launders
  • Continuous Casting Level Feed Tundishes
  • Other preformed shapes for molten aluminum applications

Advantages

  • Resistant to thermal shock
  • Does not require the application of aluminum resistant coating
  • Does not contain alumina silicate refractory ceramic fibers
  • Light weight
  • Does not require a supporting steel shell in certain applications such as continuous casting launders
  • Reusable for multiple casts

Information provided by Pyrotek.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 0.594 g/cc
Loss On Ignition 0.55 %
@Temperature 900 °C
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.00237 GPa
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.160 W/m-K
@Temperature 540 °C
 0.190 W/m-K
@Temperature 815 °C
Maximum Service Temperature, Air 850 °CContinuous
 1000 °C
Shrinkage 0.11 %
@Temperature 400 °C
 0.80 %
@Temperature 730 °C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Pyrotek O'-Sialon Non-Oxide Ceramic
Pyrotek S-679 Dense Graphite Material Treated for Oxidation Resistance
Pyrotek Valcor® G Pre-Cast Shapes
Pyrotek Valcor® G-AZ Pre-Cast Shapes
Pyrotek Pyroboard™ S1090 Roller

CPYRO200 / 1917

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.