MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
M50-NiL High Performance Carburizing Bearing and Gear Steel
Categories: Metal; Ferrous Metal; Alloy Steel; Carbon Steel; High Carbon Steel

Material Notes: A carburizing bearing and gear steel designed for service temperatures up to 600°F. The chemistry is engineered such that when suitably carburized and heat treated the case will have a microstructure of fine tempered martensite with an even distribution of fine carbides. Improved over conventional through hardening M50 is the relatively high fracture toughness properties of the core. Because the alloy can be carburized, surface stresses can be controlled to provide excellent rolling contact fatigue characteristics.

Information provided by Latrobe and the reference(s).

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.284 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 29500 ksi
Fracture Toughness 29.0 - 33.0 ksi-in½cracks originating in case; case depth 0.30 to 0.35 in.
 38.0 - 45.0 ksi-in½cracks originating in core
Charpy Impact 30.0 - 50.0 J
@Temperature -17.8 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 11.2 µm/m-°C
@Temperature 21.0 - 204 °C
 12.0 µm/m-°C
@Temperature 21.0 - 427 °C
Maximum Service Temperature, Air 600 °F
Transformation Temperature 215 °CMartensitic Finish
 332 °CMartensitic Start
 
Processing PropertiesOriginal ValueComments
Processing Temperature 738 °CCritical Temperature Core Ac1
 960 °CCritical Temperature Core Ac3
 
Component Elements PropertiesOriginal ValueComments
Carbon, C 0.13 %
Chromium, Cr 4.2 %
Iron, Fe 86.37 %
Manganese, Mn 0.25 %
Molybdenum, Mo 4.25 %
Nickel, Ni 3.4 %
Silicon, Si 0.20 %
Vanadium, V 1.2 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AISI Type M50 Tool Steel
Latrobe Lescalloy® M50 VIM-VAR High Performance Bearing Steel
Latrobe CM-50™ ASTM M50 High Speed Steel
Latrobe Lescalloy® 52100 VAC-ARC High Performance Bearing Steel
AISI E 52100 Steel (100Cr6, SUJ2, UNS G52986)

MQZ9943 / 172240

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.