System Message
Advertise with MatWeb!
Data sheets for over
180,000
metals, plastics, ceramics, and composites.
HOME
•
SEARCH
•
TOOLS
•
SUPPLIERS
•
FOLDERS
•
ABOUT US
•
FAQ
•
LOG IN
Recently Viewed Materials (most recent at top)
Login
to see your most recently viewed materials here.
Or if you don't have an account with us yet, then
click here to register.
Searches:
Advanced
|
Category
|
Property
|
Metals
|
Trade Name
|
Manufacturer
|
Recently Viewed Materials
(Viewing data as-entered.
Click here
to return)
A. Schulman Diamond ASA M-143
Categories:
Polymer
;
Thermoplastic
;
ASA Polymer
;
Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
Material Notes:
Description:
ASA Weatherable Polymer, Injection Molding Grade, High Heat
Information provided by Diamond Polymers, Inc.
A. Schulman has acquired Network Polymers & Diamond Polymers.
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Specific Gravity
1.10
g/cc
ASTM D792
Linear Mold Shrinkage
0.0040
-
0.0070
cm/cm
ASTM D955
Melt Flow
4.4
g/10 min
@Load 5.00 kg,
Temperature 200 °C
Procedure A Condition G; ASTM D1238
Mechanical Properties
Original Value
Comments
Tensile Strength, Yield
7672
psi
chs 2 in/min; ASTM D638
Flexural Strength
11600
psi
chs 0.05 in/min; ASTM 790
Flexural Modulus
355000
psi
Tangent, chs 0.05 in/min; ASTM D790
Izod Impact, Notched
1.70
ft-lb/in
@Thickness 3.17 mm,
Temperature 23.0 °C
bar; ASTM D256
Thermal Properties
Original Value
Comments
Deflection Temperature at 1.8 MPa (264 psi)
203
°F
0.125 in bar Unannealed/Conditioned 40 hours at 23°C; ASTM D648
217
°F
0.25 in bar Unannealed/Conditioned 40 hours at 23°C; ASTM D648
Vicat Softening Point
248
°F
0.125 inch, 1 Kg; ASTM D1525
Optical Properties
Original Value
Comments
Gloss
96.5 %
at 60°; ASTM D523
Processing Properties
Original Value
Comments
Rear Barrel Temperature
480
-
490
°F
Middle Barrel Temperature
500
-
510
°F
Front Barrel Temperature
510
-
520
°F
Nozzle Temperature
510
-
520
°F
Melt Temperature
430
-
520
°F
Melt temperatures above 530°F are not recommended, and may result in color shifts and or thermal instability.
Mold Temperature
170
-
180
°F
Higher mold temperature can aid flow in processing, provides a better surface finish, and creates less residual stress in the finished products.
Drying Temperature
180
-
198
°F
Dry Time
4
-
6
hour
Moisture Content
<= 0.10 %
Back Pressure
75.0
-
150
psi
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
A. Schulman Diamond ASA 91802
A. Schulman Diamond ASA 5946
A. Schulman Diamond ASA S150
A. Schulman Diamond ASA S210B
A. Schulman Diamond ASA S510
PDIAM267 / 30105
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.