(Viewing data as-entered.
Click here
to return)
3M Jet-melt™ 3731 Polyolefin Bonding Adhesive
Categories:
Polymer
;
Adhesive
Material Notes:
3M™ Jet-Melt™ Polyolefin Bonding Adhesive 3731 is 100% solids, high heat resistant adhesive that bonds to a variety of substrates including polyethylene and many other plastics.
Information provided by 3M
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.920
g/cc
Brookfield Viscosity
12000
cP
#276 sp @ 10 rpm
Mechanical Properties
Original Value
Comments
Shear Strength
257
psi
Overlap, Polystyrene (High Impact)
390
psi
Overlap, Cold Rolled Steel
420
psi
Overlap, HDPE
430
psi
Overlap, PVC (Rigid)
430
psi
Overlap, Polycarbonate
450
psi
Overlap, ABS
475
psi
Overlap, Nylon 66
490
psi
Overlap, Douglas Fir
550
psi
Overlap, Polypropylene
Impact Test
80.0
in-lb
Peel Strength
15.0
pli
180° Canvas to Polystyrene (High Impact)
15.0
pli
180° Canvas to Cold Rolled Steel
18.0
pli
180° Canvas to PVC (Rigid)
19.0
pli
180° Canvas to Nylon 66
22.0
pli
180° Canvas to Polypropylene
22.0
pli
180° Canvas to Polycarbonate
23.0
pli
180° Canvas to HDPE
23.0
pli
180° Canvas to ABS
Thermal Properties
Original Value
Comments
Flash Point
273
°C
COC
Ring & Ball Softening Point
157
°C
ASTM E28-607
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
PMM34079 / 168826
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.