MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Momentive Performance Materials BIN77 Aluminum Nitride/ Boron Nitride Composite  (discontinued **)
Categories: Ceramic; Ceramic Matrix Composite; Nitride

Material Notes: Boron Nitride is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mullite and Titanium Diboride. This results in composites which are machinable, thermal shock resistant, and chemically compatible in a wide range of environments. In combination with Titanium Diboride, for example, BN can be used as a heating source for the aluminum metallization of films and papers. BN composites are also used as break-rings in the horizontal continuous castings of steel and nozzles in rapid solidification processes. Other composite applications include the following:
  • High temperature refractory shapes
  • Glass forming tools and refractories
  • Molds, dies and refractories for metalforming
  • Furnace vents, stacks and fixtures

Information provided by Momentive Performance Materials, formerly GE Advanced Ceramics.

Key Words: BN, AlN
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 2.43 g/cc
 
Mechanical PropertiesOriginal ValueComments
Modulus of Elasticity 4000 - 9000 ksiSonic Modulus
Flexural Strength 18000 psi
 4000 psi
@Temperature 1500 °C
 
Thermal PropertiesOriginal ValueComments
CTE, linear 5.00 - 6.00 µm/m-°C
@Temperature 20.0 °C
Thermal Conductivity 25.0 - 40.0 W/m-K

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aremco AREMCOLOX™ 502-1800 Machinable Aluminum Nitride
American Elements Aluminum Nitride Nanoparticles
Aluminum Nitride, AlN
MarkeTech AN 180 Aluminum Nitride Ceramic Substrate, 99% Purity
MarkeTech AN 90 Aluminum Nitride Ceramic Substrate, 98% Purity

CADV53 / 437

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.