(Viewing data as-entered.
Click here
to return)
Von Roll Isola IMI Varnish 9637AP Polyester Varnish for Electrical Insulation
Categories:
Polymer
;
Thermoset
;
Polyester, TS
;
Thermoset Polyester Solventless Electrical Varnish
Material Notes:
Data provided by Von Roll Isola USA.
Flash Point: 53°C. Average solids: 48%. Usage Notes: Higher flash point version of IMI 9637
Key Words:
Von Roll Isola USA; Insulating Materials Incorporated
Vendors:
No vendors are listed for this material. Please
click here
if you are a supplier and would like information on how to add your listing to this material.
Printer friendly version
Download as PDF
Download to Excel (requires Excel and Windows)
Export data to your CAD/FEA program
Add to Folder:
My Folder
Physical Properties
Original Value
Comments
Density
0.970
g/cc
Viscosity
240
cP
Electrical Properties
Original Value
Comments
Dielectric Strength
122
kV/mm
Thermal Properties
Original Value
Comments
Maximum Service Temperature, Air
180
°C
Processing Properties
Original Value
Comments
Processing Temperature
150
°C
Suggested baking time at this temperature is 1-6 hr.
Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's
terms of use
regarding this information.
Click here
to go back to viewing the property data in MatWeb's normal format.
Users viewing this material also viewed the following:
Von Roll Isola IMI Varnish 9637 Polyester Varnish for Electrical Insulation
Von Roll Isola IMI Varnish 9522 Polyester Varnish for Electrical Insulation
Von Roll Isola IMI Varnish 707 Solventless Polyester Varnish for Electrical Insulation
Von Roll Isola IMI Varnish 704 Solventless Polyester Varnish for Electrical Insulation
Von Roll Isola IMI Varnish 702 Solventless Polyester Varnish for Electrical Insulation
PISO26 / 48429
Subscribe to Premium Services
Searches:
Advanced
•
Composition
•
Property
•
Material Type
•
Manufacturer
•
Trade Name
•
UNS Number
Other Links:
Advertising
•
Submit Data
•
Database Licensing
•
Web Design & Hosting
•
Trade Publications
Supplier List
•
Unit Converter
•
Reference
•
Links
•
Help
•
Contact Us
•
Site Map
•
FAQ
•
Home
Follow @MatWeb
Please read our
License Agreement
regarding materials data and our
Privacy Policy
. Questions or comments about MatWeb? Please contact us at
webmaster@matweb.com
. We appreciate your input.
The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.