MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
LyondellBasell Petrothene® NA443023 Blown Low Density Polyethylene
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: Applications
PETROTHENE NA 443 is a series of low density/EVA copolymer resins for high impact/high clarity packaging applications. NA 443 exhibits excellent processability and good balance of optics and strong heat sealing characteristics.

Regulatory Status
NA 443 meets the requirements of the Food and Drug Administration regulation 21 CFR 177.1350. This regulation allows the use of this ethylene vinyl acetate copolymer "…in articles or components of articles intended for use in contact with food." Specific limitations or conditions of use may apply.

Processing Techniques
NA 443 has excellent drawdown characteristics that yield outstanding output rates. Optimum properties are obtained over a broad range of extrusion conditions at melt temperatures between 330°-380°F melt temperatures and a blow-up ratio between 1.7-3.0:1. Using proper techniques and equipment, NA 443 can be drawn to 1.0 mil at commercial production rates. Specific recommendations for the processing of NA 442 can be made only when the end use application, required properties and the processing equipment are known.

Physical Properties
These are typical values and not to be construed as specific product limits. Data obtained from film produced in a 3.5"(89mm) blown film line, commercially available 8"(203 mm)die, 375°F(191°C) melt extrusion temperature, 2:1 BUR, 1.25 mil (32 micron) gauge, 0.025"die gap at 130 lb/hr.

This product is from the former Equistar product line.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.927 g/ccASTM D1501
Vinyl Acetate Content 4.5 %
Thickness 1.25 mil2:1 BUR; 25 mil die gap
Melt Flow 1.2 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Film Elongation at Break, MD 350 %ASTM D882
Film Elongation at Break, TD 550 %ASTM D882
Elmendorf Tear Strength MD 140 gASTM D1922
Dart Drop Test 150 gF50; ASTM D1709
Film Tensile Strength at Break, MD 4000 psiASTM D882
Film Tensile Strength at Break, TD 2900 psiASTM D882
1% Secant Modulus, MD 20000 psiASTM D882
1% Secant Modulus, TD 18000 psiASTM D882
 
Thermal PropertiesOriginal ValueComments
Vicat Softening Point 88.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 3.0 %ASTM D1003
Gloss 77 %at 45°; ASTM D2457
 
Processing PropertiesOriginal ValueComments
Melt Temperature 375 °F
 
Compliance PropertiesOriginal ValueComments
FDA YesSee notes for details.
 
Descriptive Properties
AntiblockNone
SlipNone

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
LyondellBasell Petrothene® NA340013 Low Density Polyethylene
Overview of materials for Low Density Polyethylene (LDPE), Molded
LyondellBasell Petrothene® NA340185 Low Density Polyethylene, Film Extrusion Grade
Versalis Riblene® FH 10 Low Density Polyethylene - Blown Film Extrusion
Versalis Riblene® FC 40 Low Density Polyethylene - Blown Film Extrusion

PEQU0491 / 36947

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.