MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Hogen Duralloy H5TC 50 Tungsten Carbide/50 Copper PM Metal Composite
Categories: Metal; Metal Matrix Composite; Nonferrous Metal; Copper Alloy; Refractory Metal; Tungsten Alloy

Material Notes: Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.

Typical Resistance Welding Applications: Used for light duty projection welding dies requiring low pressure. Another common use is tips on contact shoe facings used in high frequency continuous welding processes. Same general uses as Hogen H5W, but with higher wear resistance.

Data provided by Hogen Industries.

Key Words: Hogen Industries Powder Metallurgy Metal Composite; Copper Alloys; WC
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density >= 11.0 g/cc
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell B 90
Tensile Strength, Ultimate 483 MPa
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000370 ohm-cm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 12.2 µm/m-°C
@Temperature 20.0 °C
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 50 %
WC 50 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Aperam Resistohm® 125 Resistant Alloys Iron-Chromium-Aluminium Alloys
Hogen Duralloy H10TC 56 Tungsten Carbide/44 Copper PM Metal Composite
AISI Type S5 Tool Steel, austenitized 855-870°C (1575-1600°F), oil quenched to 55 HRC
Aperam Resistohm® 145 Resistant Alloys Iron-Chromium-Aluminium Alloys
Beryllium I-70H, Optical Grade

NHOG17 / 17325

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.