MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC VALOX™ FR Resin ENH3500 Polybutylene Terephthalate (PBT) (Europe)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT); Polybutylene Terephthalate (PBT), Unreinforced, Molded

Material Notes: VALOX ENH3500 is an unreinforced, non-chlorinated/brominated flame retardant Polybutylene Terephthalate (PBT) injection moldable grade with excellent chemical resistance. It has a UL94V0@0.80mm flame rating. This is a good candidate for a variety of applications needing a sustainable FR PBT solution.

Features: Chemical Resistance,Flame Retardant,Non-Chlorinated,Non-Brominated,ECO Compliant

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D792
Density 1.31 g/ccISO 1183
Water Absorption 0.35 %
@Time 86400 sec
ASTM D570
Moisture Absorption 0.0200 %Injection Molding
 0.0800 %23°C/50% RH/24 hrs; ASTM D570
 0.0800 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 0.35 %ISO 62-1
Viscosity 20 cP
@Load 2.16 kg,
Temperature 250 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.018 - 0.028 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 38.0 MPa50 mm/min; ISO 527
 42.0 MPa50 mm/min; ASTM D638
Tensile Strength, Yield 39.0 MPa50 mm/min; ISO 527
 44.0 MPa50 mm/min; ASTM D638
Elongation at Break 8.0 %50 mm/min; ISO 527
 10 %50 mm/min; ASTM D638
Elongation at Yield 3.0 %50 mm/min; ASTM D638
 3.0 %50 mm/min; ISO 527
Tensile Modulus 3150 MPa5 mm/min; ASTM D638
 3200 MPa1 mm/min; ISO 527
Flexural Strength 70.0 MPayield, 2 mm/min; ISO 178
 77.0 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
Flexural Modulus 2700 MPa2 mm/min; ISO 178
 2750 MPa1.3 mm/min, 50 mm span; ASTM D790
Izod Impact Notched 40.0 JASTM D256
Izod Impact, Unnotched NBASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) NB80*10*4; ISO 180/1U
 NB
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched NBEdgew 80*10*4 sp=62mm; ISO 179/1eU
Charpy Impact, Notched 6.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
 >= 1.00e+15 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Comparative Tracking Index 600 VIEC 60112
 >= 600 VUL 746A
Hot Wire Ignition, HWI 7.0 - 15 sec
@Thickness >=0.800 mm
UL 746A
 15 - 30 sec
@Thickness >=1.50 mm
UL 746A
 30 - 60 sec
@Thickness >=3.00 mm
UL 746A
High Amp Arc Ignition, HAI >= 120 arcs
@Thickness >=0.800 mm
UL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature -40.0 - 95.0 °C
ASTM E831
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 160 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 160 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 60.0 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 60.0 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 170 °CRate B/50; ASTM D1525
 170 °CRate B/120; ISO 306
 170 °CRate B/50; ISO 306
UL RTI, Electrical 150 °CUL 746B
UL RTI, Mechanical with Impact 105 °CUL 746B
UL RTI, Mechanical without Impact 150 °CUL 746B
Flammability, UL94 V-0
@Thickness >=0.800 mm
UL 94
 5VB
@Thickness >=2.00 mm
UL 94
 5VA
@Thickness >=3.00 mm
UL 94
Oxygen Index 31 %ASTM D2863
 31 %ISO 4589
Glow Wire Ignition Temperature 700 °C
@Thickness 1.50 mm
IEC 60695-2-13
 700 °C
@Thickness 2.00 mm
IEC 60695-2-13
 700 °C
@Thickness 3.00 mm
IEC 60695-2-13
 750 °C
@Thickness 0.800 mm
IEC 60695-2-13
Glow Wire Flammability Index 960 °C
@Thickness 0.800 mm
IEC 60695-2-12
 960 °C
@Thickness 1.50 mm
IEC 60695-2-12
 960 °C
@Thickness 2.00 mm
IEC 60695-2-12
 960 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 230 - 255 °C
Zone 2 235 - 250 °C
Zone 3 240 - 260 °C
Melt Temperature 245 - 260 °CInjection Molding
Mold Temperature 40.0 - 100 °C
Drying Temperature 110 - 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Precipitation Temperature 40.0 - 60.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82774 / 290721

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.