MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
SABIC NORYL GTX™ Resin GTX918W Polyphenylene Ether + PA (PPE+Nylon) (Europe)
Categories: Polymer; Thermoplastic; Nylon (Polyamide PA); Polyphenylene Ether/PPO

Material Notes: NORYL GTX™ 918W resin is a non-reinforced alloy of Polyphenylene Ether (PPE) + Polyamide (PA). This injection moldable grade exhibits high heat resistance, excellent chemical resistance, and high melt flow. NORYL GTX918W resin may be an excellent candidate for automotive under-the-hood and electrical applications requiring the retention of properties while under thermal load.

Features: Hydrolytic Stability,Low Creep Sensitivity,Good Stiffness,Low Warpage,High Flow,Good Processability,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.10 g/ccISO 1183
Moisture Absorption 0.0700 %Injection Molding
 1.34 %23°C / 50% RH; ISO 62
Water Absorption at Saturation 4.2 %ISO 62-1
Viscosity 5.0 cP
@Load 1.20 kg,
Temperature 280 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.016 - 0.020 cm/cmSABIC method
 
Mechanical PropertiesOriginal ValueComments
Ball Indentation Hardness 95.0 MPaH358/30; ISO 2039-1
Tensile Strength at Break 55.0 MPa50 mm/min; ISO 527
Tensile Strength, Yield 60.0 MPa50 mm/min; ISO 527
Elongation at Break 30 %50 mm/min; ISO 527
Elongation at Yield 4.5 %50 mm/min; ISO 527
Tensile Modulus 2400 MPa1 mm/min; ISO 527
Flexural Strength 85.0 MPayield, 2 mm/min; ISO 178
Flexural Modulus 2200 MPa2 mm/min; ISO 178
Izod Impact, Notched (ISO) 20.0 kJ/m²80*10*4; ISO 180/1A
 10.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Charpy Impact, Notched 20.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 10.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 80.0 µm/m-°C
@Temperature 23.0 - 60.0 °C
ISO 11359-2
Thermal Conductivity 0.250 W/m-KISO 8302
Hot Ball Pressure Test 125 °CPASS; IEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 185 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
Vicat Softening Point 190 °CRate B/50; ISO 306
 195 °CRate B/120; ISO 306
 245 °CRate A/50; ISO 306
UL RTI, Electrical 120 °CUL 746B
UL RTI, Mechanical with Impact 110 °CUL 746B
UL RTI, Mechanical without Impact 125 °CUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 270 - 300 °C
Zone 2 270 - 290 °C
Zone 3 280 - 300 °C
Melt Temperature 280 - 310 °CInjection Molding
Mold Temperature 80.0 - 120 °C
Drying Temperature 100 - 120 °CInjection Molding
Dry Time 2.00 - 3.00 hourInjection Molding
Precipitation Temperature 60.0 - 80.0 °CHopper Temperature

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82168 / 290115

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.