MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Vibrantz Technologies IX 2730 Passivation Glasses - High Voltage (Zn-B-Silicates)
Categories: Ceramic; Glass; Oxide; Silicon Oxide

Material Notes: Typical Powder Form: TF

Zinc-Boro-Silicate passivation glasses are used for hermetic passivation of high voltage diodes, thyristors, and transistors. They provide high junction temperatures and can be applied to wafers using thick film and electrophoresis methods. These products are formulated and produced to achieve low alkali and iron levels. These glasses are also used for encapsulation of rectifiers using glass beading application methods. IX 2730 is a crystallizing glass that when fired, closely matches the expansion of silicon for use on stacked-chip diodes for high voltage devices.

Information provided by Ferro Corporation

Ferro Corporation is now a part of Vibrantz Technologies.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 3.90 g/cc
Particle Size 10 µm50% of particles
 <= 75 µm
 
Chemical PropertiesOriginal ValueComments
Ionic Impurities - Na (Sodium) <= 20 ppm
Ionic Impurities - K (Potassium) <= 10 ppm
 
Thermal PropertiesOriginal ValueComments
CTE, linear 3.70 µm/m-°Cat Set Pt.; Crystallized
 4.40 µm/m-°C
@Temperature 260 °C
Crystallization Temperature 715 °C
Softening Point 615 °C
Transformation Temperature 540 °C
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 175 °CMaximum Junction Temperature
 720 °CTypical Firing Temperature; Typical Firing Time: 10-15 min.
 
Descriptive Properties
Ionic Impurities - Li (Lithium) ppm, Max10

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borosilicate Glass
Beryllium Aluminum Metasilicate, Be3Al2(SiO3)6
Barium Metasilicate, BaSiO3
Barium Disilicate, BaSi2O5
Augite (Iron-Magnesium Silicate)

CFERR46 / 860

New MatWeb Services

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.