MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
BYK ADD-VANCE® TH 130 Stabilization Masterbatch, PP base  (discontinued **)
Categories: Other Engineering Material; Additive/Filler for Polymer; Polymer; Thermoplastic; Polypropylene (PP)

Material Notes: Fields of application: Stabilization and processing master batch for producing glass mat reinforced polypropylene (GMT) and long fiber reinforced PP materials (LFTs).
Examples: Long fiber reinforced materials for automotive parts, like undercover shields, dashboard carriers, assembly carriers, front panels, front bumpers etc.

Mode of action and advantages: ADD-VANCE® TH 130 contains a synergistic blend of processing stabilizers and heat stabilizers. Processing stabilizers protect the polymer during processing operations at high temperature by decomposing reactive hydroperoxides. Heat stabilizers inhibit the thermo-oxidative degradation of the end-product by radical scavenging reactions.

Advantages: Excellent Long Term Heat Ageing (LTHA) to achieve VW and D-C requirements; Good glueing properties; Non-blooming additives and low emission of organic compounds from finished part; High accuracy in dosing of each individual additive component in ADD-VANCE® TH 130 to ensure product consistency and a guaranteed, defined composition in the final product; Optimized combination of additives to achieve lower overall costs and easy processing; Non-sticking pellets, dust free dosing; Safe and easy handling.

Former ADDCOMP product line, acquired by BYK.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.500 - 0.650 g/cc
 
Processing PropertiesOriginal ValueComments
Processing Temperature <= 300 °C
 
Descriptive Properties
AppearanceWhite to off-white granules
Dosing Level2-4%

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PPADDC27 / 133240

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.