MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
SABIC NORYL™ Resin GFN2 Polyphenylene Ether + PS (PPE+PS) (Americas)
Categories: Polymer; Thermoplastic; Polystyrene (PS); Polystyrene + Polyphenylene Ether, Unreinforced

Material Notes: NORYL™ GFN2 resin is a 20% glass reinforced blend of polyphenylene ether (PPE) + high impact polystyrene (HIPS). This general-purpose injection moldable grade exhibits very low moisture absorption, high strength, hydrolytic stability, Low warpage, low specific gravity, and dimensional stability. NORYL GFN2 carries a UL746C outdoor suitability rating of F1 and is an excellent candidate for a variety of indoor and outdoor applications including construction, electrical components + displays, lawn and garden equipment. *See NORYL GFN2F resin for FDA food compliant / NSF version.

Features: Hydrolytic Stability,Low Warpage,Structural

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.20 g/ccASTM D792
Water Absorption 0.060 %
@Time 86400 sec
ASTM D570
Moisture Absorption 0.0200 %Injection Molding
Viscosity 8.0 cP
@Load 5.00 kg,
Temperature 300 °C
MVR cc/10 min; ISO 1133
Linear Mold Shrinkage, Flow 0.0020 - 0.0050 cm/cm
@Thickness 3.20 mm
SABIC method
Melt Flow 9.0 g/10 min
@Load 5.00 kg,
Temperature 300 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell L 106ASTM D785
Tensile Strength at Break 90.0 MPa5 mm/min; ASTM D638
 97.0 MPa5 mm/min; ISO 527
Elongation at Break 2.5 %5 mm/min; ISO 527
 2.6 %5 mm/min; ASTM D638
Tensile Modulus 6200 MPa5 mm/min; ASTM D638
 7070 MPa1 mm/min; ISO 527
Flexural Strength 160 MPayld, 1.3 mm/min, 50 mm span; ASTM D790
 167 MPayield, 2 mm/min; ISO 178
Flexural Modulus 5800 MPa1.3 mm/min, 50 mm span; ASTM D790
 6540 MPa2 mm/min; ISO 178
Izod Impact Notched 119 JASTM D256
 96.0 J
@Temperature -40.0 °C
ASTM D256
Izod Impact, Unnotched 650 J/mASTM D4812
Izod Impact, Notched (ISO) 11.0 kJ/m²80*10*4; ISO 180/1A
Charpy Impact, Notched 11.0 kJ/m²ISO 179/2C
Dart Drop, Total Energy 22.0 JASTM D3763
 
Electrical PropertiesOriginal ValueComments
Dielectric Constant 2.86
@Frequency 50.0 - 60.0 Hz
ASTM D150
Dielectric Strength 16.5 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
Dissipation Factor 0.00080
@Frequency 50.0 - 60.0 Hz
ASTM D150
Arc Resistance 0.00 - 60 secASTM D495
Hot Wire Ignition, HWI 7.0 - 15 sec
@Thickness >=1.50 mm
UL 746A
 60 - 120 sec
@Thickness >=6.00 mm
UL 746A
High Amp Arc Ignition, HAI 0.00 - 15 arcs
@Thickness >=1.50 mm
UL 746A
 15 - 30 arcs
@Thickness >=6.00 mm
UL 746A
High Voltage Arc-Tracking Rate, HVTR >= 150 mm/minUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 33.0 µm/m-°C
@Temperature -40.0 - 90.0 °C
ASTM E831
 33.0 µm/m-°C
@Temperature -40.0 - 90.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 90.0 µm/m-°C
@Temperature -40.0 - 90.0 °C
ASTM E831
 90.0 µm/m-°C
@Temperature -40.0 - 90.0 °C
ISO 11359-2
Deflection Temperature at 0.46 MPa (66 psi) 143 °CEdgew 120*10*4 sp=100mm; ISO 75/Be
 140 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 143 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 137 °CEdgew 120*10*4 sp=100mm; ISO 75/Ae
 135 °C
@Thickness 3.20 mm
unannealed; ASTM D648
 137 °C
@Thickness 6.40 mm
unannealed; ASTM D648
Vicat Softening Point 143 °CRate B/50; ISO 306
 146 °CRate B/120; ISO 306
UL RTI, Electrical 90.0 °CUL 746B
UL RTI, Mechanical with Impact 90.0 °CUL 746B
UL RTI, Mechanical without Impact 90.0 °CUL 746B
Flammability, UL94 HB
@Thickness >=1.50 mm
UL 94
Oxygen Index 26 %ASTM D2863
 
Processing PropertiesOriginal ValueComments
Nozzle Temperature 300 - 325 °C
Zone 2 275 - 320 °C
Zone 3 290 - 325 °C
Melt Temperature 300 - 325 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 110 - 120 °CInjection Molding
Dry Time 3.00 - 4.00 hourInjection Molding
 8.00 hourCumulative; Injection Molding
Back Pressure 0.300 - 0.700 MPa
Shot Size 30 - 70 %
Screw Speed 20 - 100 rpm
 
Descriptive Properties
UV-light, water exposure/immersionF1UL 746C

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH82312 / 290259

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.