BC7136-2 is an aluminum filled thick section casting system with heat resistance to 300ºF. May be cast to a thickness of 2 inches in non-conductive molds, 3 inches in conductive molds and thicker sections with the addition of bulk fill. For service temperature above 150ºF a post-cure is required. Does not contain VCHD or MDA. See cure schedule.Information provided by BCC Products, Inc. |