MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Lion Royalene® 677 EPDM
Categories: Polymer; Thermoset; Rubber or Thermoset Elastomer (TSE)

Material Notes: A Highly Extendable ENB Polymer with Heavy Hydrotreated Paraffinic Oil for TPO/TPV and Thermoset Applications

Unique Features:

  • Blends readily with polyolefins for TPO and TPV compounds
  • Provides enhanced compression set and good color in TPV
  • Highly extendable
  • Good aging properties
  • Good shape retention in extruded applications
  • Very high molecular weight base polymer
  • High green strength over a broad temperature range
  • Useful for making low hardness compounds
  • Extended with a white, hydrotreated paraffinic oil
Applications:
  • TPO and TPV
  • Automotive applications
  • Mechanical goods
  • Hose, tubes, Profile extrusions

Information provided by Lion Elastomer

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 0.880 g/ccASTM D-792
Volatiles <= 1.0 %ZS 1008K
Mooney Viscosity 50
@Temperature 125 °C
ML (1+4), Unmilled; ZS 1220B
 
Descriptive Properties
ColorOff-whiteZS 1072A
Content4.5ENB, ZS 1222
Oil Extension100 phrHydrotreated Paraffinic, ZS 1297
StabilizerNon-Staining
Weight Ratio70/30E/P, ZS 1231

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PLION018 / 317927

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.