MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Nouryon Ethomeen T/24 Polyoxyethylene (14) Tallowalkyamines
Categories: Other Engineering Material

Material Notes: Ethomeen T/24 is a tallow amine ethoxylates with 14 moles of ethylene oxide.

Information provided by Nouryon

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.024 g/cc
pH 10 - 10.61% in DI water
Vapor Pressure <= 0.000130 bar
@Temperature 20.0 °C
 <= 0.00130 bar
@Temperature 200 °C
Surface Tension 40 dynes/cm1.0% solution
 41 dynes/cm0.1% solution
 41.6 dynes/cmat 0.5% and 25°C
 
Thermal PropertiesOriginal ValueComments
Melting Point -3.00 °C
Boiling Point >= 300 °C
@Pressure 0.101325 MPa
Initial
Pour Point -1.00 °C
Flash Point >= 100 °C
 
Optical PropertiesOriginal ValueComments
Gardner Color Number 8.0 - 12
 
Component Elements PropertiesOriginal ValueComments
H2O, Water <= 1.0 %
 
Descriptive Properties
Amine number61.2 - 65.1 mg KOH/g
AppearanceLiquid
Cloud point=100°C1% in water
Equivalent mass890 g/eq
HLB14Davies Scale 0-40

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PNOURY538 / 286061

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.