ELASTOSIL® R plus 4305/80 is a platinum-catalyzed addition-curing, two-part silicone rubber for manufacturing extruded articles. Cured articles show an excellent transparency and good to very good mechanical properties. Application: ELASTOSIL® R plus 4305/80 is suitable for use under the Recommendation XV. Silicones of the BfR and FDA 21 CFR §177.2600 "Rubber Articles Intended for Repeated Use" provided that the product is appropriately cured/ post-cured and the respective limits for extractable/migrating or volatile components are met. Information provided by Wacker Chemie AG. |