MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Dielectric Polymers NT-1020 Silicone/Acrylic Double Coated Tape  (discontinued **)
Categories: Polymer; Adhesive; Tape; Thermoset; Silicone

Material Notes: Crosslinked silicone and acrylic adhesive with 2 mil polyester film release liner backing on the silicone side and moisture stable PE coated kraft (60#) on the acrylic side.

Features:

  • Chemical resistant
  • High Temperature resistant
  • Good conformability
  • High adhesion
  • Solvent resistant
  • Plasticizer migration resistant - acrylic side
  • Bonds well to LSE substrates - silicone side

Applications:

Overlap splicing and laminating various silicone surfaces such as silicone foam, rubber and gaskets to non-silicone coated substrates.

Information provided by Dielectric Polymers.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Thickness 1.00 milPET Carrier
 2.00 milAcrylic
 2.00 milSilicone
 
Mechanical PropertiesOriginal ValueComments
Peel Strength 2.875 pliAdhesion, acrylic side
 3.4375 pliAdhesion, silicone side
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 350 °FAcrylic side
 450 °FIntermittent, acrylic side
 450 °FShear Adhesive Failure (cohesive failure) - acrylic side
 >= 500 °FShear Adhesive Failure (polyester failure) - silicone side
 500 °FSilicone side
 700 °FIntermittent, silicone side
Minimum Service Temperature, Air -300 °FSilicone side
 -40.0 °FAcrylic side
 
Descriptive Properties
ColorTranslucent
Tensile StrengthRoom Temp. Shear, PET/s.s.: >167 hours - silicone side / 350°F shear: 1"x1"x1000 gr., PET/s.s.: >24 ours - acrylic side

**
Materials flagged as discontinued () are no longer part of the manufacturer’s standard product line according to our latest information. These materials may be available by special order, in distribution inventory, or reinstated as an active product. Data sheets from materials that are no longer available remain in MatWeb to assist users in finding replacement materials.

Users of our Advanced Search (registration required) may exclude discontinued materials from search results.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Rogers Arlon E950-10RXX-M8 0.050" (1.27 mm) Cured Silicone Rubber with PSA liner
Resin Technology Group 310 Porous Fill, Slow Set Fusion™ Cyanoacrylate Instant Ethyl Adhesive
Permabond HM165 Anaerobic Retainer
Permabond 922 Cyanoacrylate, High temperature
Dielectric Polymers NT-490 Polyimide Label Stock

PDIEL19 / 30134

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.