MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper Alloy, UNS C44730, H08 Temper, Flat Products & Rod
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Spring

Fabrication Properties: Excellent Suitability – Brazing, Spot Weld; Good Suitability – Soldering, Oxyacetylene Welding, Butt Weld, Capacity for Being Cold Worked; Fair Suitability – Gas Shielded Arc Welding, Capacity for Being Hot Formed

Typical Uses: Electrical Connectors – Automotive; Automotive Electronic Connectors; Conductors, Electrical and Thermal, High Strength

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.308 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength 117 ksiTypical
 111 - 124 ksi
Tensile Strength, Yield >= 100 ksi0.2% Offset
 107 ksi0.2% Offset, Typical
Elongation at Break 1.0 %
Poissons Ratio 0.34
Machinability 40 %
Forgeability 75 %
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000820 ohm-cm21% IACS
Magnetic Permeability 1.0
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 67.0 BTU-in/hr-ft²-°F
Melting Point 1700 - 1780 °F
Solidus 1700 °F
Liquidus 1780 °F
 
Component Elements PropertiesOriginal ValueComments
Chromium, Cr <= 0.70 %
Copper, Cu 61.8 - 71.6 %As Balance
Iron, Fe <= 0.60 %
Lead, Pb <= 0.050 %
Magnesium, Mg <= 0.40 %
Manganese, Mn <= 0.40 %
Nickel, Ni 0.80 - 2.5 %
Phosphorus, P <= 0.050 %
Silicon, Si 0.10 - 0.60 %
Tin, Sn 0.50 - 1.5 %
Zinc, Zn 27 - 31 %
Zirconium, Zr <= 0.40 %

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC44730x8 / 292016

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.