MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC LNP™ STAT-KON™ Compound DX99873C Polycarbonate (PC)
Categories: Polymer; Thermoplastic; Polycarbonate (PC)

Material Notes: LNP STAT-KON DX99873C compound is based on Polycarbonate (PC) resin containing 25% carbon fiber. Added features of this grade include: LNP Clean Compounding Technology, Electrically Conductive, High Flow, Dimensional Stability.

Features: LNP Clean Compound Technology,High Stiffness,Light-weight Structural,Super Strong (Carbon Fiber Filled),Good dimensional stability,High Flow,Electrically Conductive

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.29 g/ccASTM D792
Moisture Absorption 0.0200 %Injection Molding
 0.150 %23°C/50% RH/24 hrs; ASTM D570
Linear Mold Shrinkage, Flow 0.00050 cm/cm24hrs; ISO 294
 0.0010 cm/cm24hrs; ASTM D955
Linear Mold Shrinkage, Transverse 0.0040 cm/cm24hrs; ASTM D955
 0.0040 cm/cm24hrs; ISO 294
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break 99.0 MPaISO 527
 104 MPaASTM D638
Elongation at Break 1.6 %ISO 527
 1.7 %ASTM D638
Tensile Modulus 10750 MPa50 mm/min; ASTM D638
 10800 MPa1 mm/min; ISO 527
Flexural Strength 163 MPaISO 178
 171 MPaASTM D790
Flexural Modulus 9250 MPaISO 178
 9680 MPaASTM D790
Izod Impact Notched 53.0 JASTM D256
Izod Impact, Unnotched 485 J/mASTM D4812
Izod Impact, Notched (ISO) 5.00 kJ/m²80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 30.0 kJ/m²80*10*4; ISO 180/1U
Dart Drop, Total Energy 13.0 Jpeak; ASTM D3763
Impact Test 2.00 JMultiaxial Impact; ISO 6603
 
Electrical PropertiesOriginal ValueComments
Surface Resistance 100 - 1.00e+6 ohmASTM D257
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 25.8 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 25.9 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
CTE, linear, Transverse to Flow 37.4 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 37.9 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
Deflection Temperature at 1.8 MPa (264 psi) 139 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 138 °C
@Thickness 3.20 mm
unannealed; ASTM D648
UL RTI, Electrical 80.0 °CUL 746B
UL RTI, Mechanical with Impact 80.0 °CUL 746B
UL RTI, Mechanical without Impact 80.0 °CUL 746B
Flammability, UL94 V-2
@Thickness >=1.50 mm
UL 94
 V-0
@Thickness >=3.00 mm
UL 94
 
Processing PropertiesOriginal ValueComments
Zone 2 310 - 320 °C
Zone 3 320 - 330 °C
Melt Temperature 305 - 325 °CInjection Molding
Mold Temperature 80.0 - 110 °C
Drying Temperature 120 °CInjection Molding
Dry Time 4.00 hourInjection Molding
Back Pressure 0.200 - 0.300 MPa
Screw Speed 30 - 60 rpm

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABH81275 / 289222

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.