MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Copper Alloy, UNS C70310, TM04 Temper, Flat Products
Categories: Metal; Nonferrous Metal; Copper Alloy

Material Notes: Temper: Mill-hardened Temper, TM - Hard

Fabrication Properties: Excellent Suitability – Capacity for Being Cold Worked, Capacity for Being Hot Formed; Good Suitability – Soldering, Brazing, Oxyacetylene Welding, Gas Shielded Arc Welding, Coated Metal Arc Welding, Spot Weld, Seam Weld, Butt Weld

Common Fabrication Processes: Forming and Bending; Stamping

Typical uses: Connectors; Contacts; Switches and Relays; Terminals

Applicable Specifications: Sheet & Strip – ASTM B422/B422M; Strip – ASTM B888/B88M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.319 lb/in³
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength >= 100 ksifor Standard
Tensile Strength, Yield >= 95.0 ksi0.2% Offset, for Standard
Elongation at Break 6.0 %
Tensile Modulus 18600 ksi
 
Electrical PropertiesOriginal ValueComments
Electrical Resistivity 0.00000450 ohm-cm38% IACS
 
Thermal PropertiesOriginal ValueComments
CTE, linear 9.40 µin/in-°F
@Temperature 20.0 - 100 °C
Melting Point 1957 - 1994 °F
Solidus 1957 °F
Liquidus 1994 °F
 
Component Elements PropertiesOriginal ValueComments
Copper, Cu 91.2 - 98.9 %As Balance
Iron, Fe <= 0.10 %
Lead, Pb <= 0.050 %
Magnesium, Mg <= 0.10 %
Nickel, Ni 1.0 - 4.0 %
Phosphorus, P <= 0.050 %
Silicon, Si 0.080 - 1.0 %
Silver, Ag 0.020 - 0.50 %
Tin, Sn <= 1.0 %
Zinc, Zn <= 2.0 %
Zirconium, Zr 0.0050 - 0.050 %
 
Descriptive Properties
US EPA Registered AntimicrobialYes

References for this datasheet.

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

MC70310x2 / 292422

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.