MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Borealis Borlink™ LE0592S Polyethylene
Categories: Polymer; Thermoplastic; Polyethylene (PE)

Material Notes: LE0592S is a crosslinkable black polyethylene compound, specially designed for bonded semiconductive screen applications. LE0592S is intended for semiconductive applications in XLPE high voltage and extra high voltage cables. It can be used as inner and outer semicon for bonded constructions and as inner semicon for strippable constructions. Supersmooth™ LE0592S meets these applicable requirements when processed using sound extrusion practice and testing procedure: AEIC CS8-00 (1st edition); AEIC CS7-93 (3rd edition); BS 6622; DIN VDE 0276-620; HD 620 S1; HD 632 S1; IEC 60502; IEC 60840; ISO 1872-E/BA, KHXY, 23-G200, C40; NF C33-223; NF C33-226; and UTE C 33-223.

Former trade name for this product was Supersmooth™.

Information provided by Borealis AG

Key Words: XLPE
Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 1.135 g/ccISO 1183/ISO 1872-2
Water Absorption 0.030 %Karl Fischer-titration
 
Mechanical PropertiesOriginal ValueComments
Tensile Strength at Break <= 4.40 MPaafter aging (240h, 135°C); IEC 60811-1-2
 >= 22.0 MPa25mm/min; ISO 527
Elongation at Break 200 %25mm/min; ISO 527
Tensile Set 0.00 %
@Temperature 200 °C
Permanent Deformation at 0.2 MPa after 25% elongation under load; IEC 60811-2-1
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity <= 100 ohm-cm
@Temperature 23.0 °C
ISO 3915
 <= 1000 ohm-cm
@Temperature 90.0 °C
ISO 3915
 
Processing PropertiesOriginal ValueComments
Melt Temperature 120 - 140 °C
Drying Temperature 50.0 °Chopper drying (4h)
Shelf Life 12.0 Month
 
Descriptive Properties
Göttfert Elastograph (Nm)1.14-1.38

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Borealis Borlink™ LE4244S Polyethylene Insulation Compound, Crosslinkable
Borealis Borlink™ LE4244R Polyethylene Insulation Compound, Crosslinkable
Borealis HE1878E-C2 High Molecular Weight Polyethylene, Crosslinkable
Borealis Borlink™ LE4201EHV Polyethylene Insulation Compound, Crosslinkable
Borealis Borlink™ LE4244EHV Polyethylene Insulation Compound, Crosslinkable

PBOREA594 / 108853

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.