MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
SABIC VALOX™ VX5011 PBT (Europe)
Categories: Polymer; Thermoplastic; Polyester, TP; Polybutylene Terephthalate (PBT)

Material Notes: VALOX VX5011 is a 10% glass fibre reinforced PBT+PC blend with low warpage characteristics.

Information provided by SABIC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.31 g/ccASTM D792
Density 1.31 g/ccISO 1183
Filler Content 10 %ASTM D229
Water Absorption 0.15 %23°C/sat; ISO 62
Moisture Absorption 0.100 %23°C / 50% RH; ISO 62
Viscosity 145 cP
@Shear Rate 1500 1/s,
Temperature 260 °C
melt; ISO 11443
Linear Mold Shrinkage, Flow 0.0030 - 0.0080 cm/cmSABIC method
 0.0040 - 0.0060 cm/cm
@Thickness 3.20 mm
SABIC method
Linear Mold Shrinkage, Transverse 0.0050 - 0.0090 cm/cmSABIC method
Melt Flow 18 g/10 min
@Load 3.80 kg,
Temperature 200 °C
ASTM D1238
 18 g/10 min
@Load 2.16 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 50 g/10 min
@Load 5.00 kg,
Temperature 250 °C
cm³/10 min; ISO 1133
 75 g/10 min
@Load 5.00 kg,
Temperature 265 °C
cm³/10 min; ISO 1133
 85 g/10 min
@Load 5.00 kg,
Temperature 266 °C
ASTM D1238
 85 g/10 min
@Load 5.00 kg,
Temperature 265 °C
ASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 122ISO 2039-2
Ball Indentation Hardness 165 MPaISO 2039-1
Tensile Strength at Break 90.0 MPa5 mm/min; ASTM D638
 95.0 MPa5 mm/min; ISO 527
Tensile Strength, Yield 90.0 MPa5 mm/min; ASTM D638
 95.0 MPa5 mm/min; ISO 527
Elongation at Break 3.0 %5 mm/min; ISO 527
 3.0 %5 mm/min; ASTM D638
Elongation at Yield 3.0 %5 mm/min; ISO 527
 3.0 %5 mm/min; ASTM D638
Tensile Modulus 4600 MPa5 mm/min; ASTM D638
 4700 MPa1mm/min; ISO 527
Flexural Strength 130 MPa2 mm/min; break; ISO 178
Flexural Yield Strength 126 MPa1.3 mm/min, 50 mm span; ASTM D790
 140 MPa2 mm/min; ISO 178
Flexural Modulus 3600 MPa1.3 mm/min, 50 mm span; ASTM D790
 4000 MPa2 mm/min; ISO 178
Flexural Strain at Break 5.0 %2 mm/min; ISO 178
Izod Impact, Notched 47.0 J/mASTM D256
 47.0 J/m
@Temperature 0.000 °C
ASTM D256
 47.0 J/m
@Temperature -30.0 °C
ASTM D256
Izod Impact, Unnotched 475 J/mASTM D4812
 465 J/m
@Temperature -30.0 °C
ASTM D4812
Izod Impact, Notched (ISO) 6.00 kJ/m²80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature 0.000 °C
80*10*4; ISO 180/1A
 5.00 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1A
Izod Impact, Unnotched (ISO) 40.0 kJ/m²80*10*4; ISO 180/1U
 30.0 kJ/m²
@Temperature -30.0 °C
80*10*4; ISO 180/1U
Charpy Impact Unnotched 40.0 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eU
 40.0 kJ/m²ISO 179/2C
 30.0 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eU
 40.0 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
Charpy Impact, Notched 4.00 kJ/m²Edgew 80*10*4 sp=62mm; ISO 179/1eA
 6.00 kJ/m²ISO 179/2C
 4.00 kJ/m²
@Temperature -30.0 °C
Edgew 80*10*4 sp=62mm; ISO 179/1eA
 6.00 kJ/m²
@Temperature -30.0 °C
ISO 179/2C
Dart Drop, Total Energy 37.0 JASTM D3763
Taber Abrasion, mg/1000 Cycles 54CS-17, 1 kg; SABIC method
 
Electrical PropertiesOriginal ValueComments
Volume Resistivity >= 1.00e+15 ohm-cmIEC 60093
 >= 1.00e+15 ohm-cmASTM D257
Surface Resistance >= 1.00e+15 ohmROA; IEC 60093
Dielectric Constant 3.0
@Frequency 50.0 - 60.0 Hz
IEC 60250
 3.1
@Frequency 1e+6 Hz
IEC 60250
 3.1
@Frequency 1e+6 Hz
ASTM D150
 3.2
@Frequency 100 Hz
IEC 60250
Dielectric Strength 18.0 kV/mm
@Thickness 3.20 mm
in oil; IEC 60243-1
 18.0 kV/mm
@Thickness 3.20 mm
in oil; ASTM D149
 25.0 kV/mm
@Thickness 1.60 mm
in oil; ASTM D149
 25.0 kV/mm
@Thickness 1.60 mm
in oil; IEC 60243-1
 29.0 kV/mm
@Thickness 0.800 mm
in oil; ASTM D149
 29.0 kV/mm
@Thickness 0.800 mm
in oil; IEC 60243-1
Dissipation Factor 0.0090
@Frequency 50.0 - 60.0 Hz
IEC 60250
 0.014
@Frequency 1e+6 Hz
ASTM D150
 0.014
@Frequency 1e+6 Hz
IEC 60250
 0.016
@Frequency 100 Hz
IEC 60250
Comparative Tracking Index 100 VIEC 60112
 200 VIEC 60112
Hot Wire Ignition, HWI >= 120 secUL 746A
High Amp Arc Ignition, HAI >= 120 arcsUL 746A
 
Thermal PropertiesOriginal ValueComments
CTE, linear, Parallel to Flow 36.7 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 39.4 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
 40.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 40.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
CTE, linear, Transverse to Flow 69.5 µm/m-°C
@Temperature -40.0 - 40.0 °C
ISO 11359-2
 90.0 µm/m-°C
@Temperature 23.0 - 80.0 °C
ISO 11359-2
 90.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
 148 µm/m-°C
@Temperature 23.0 - 150 °C
ISO 11359-2
Hot Ball Pressure Test 125 °CIEC 60695-10-2
Deflection Temperature at 0.46 MPa (66 psi) 135 °CFlatw 80*10*4 sp=64mm; ISO 75/Bf
 175 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 115 °CFlatw 80*10*4 sp=64mm; ISO 75/Af
 115 °C
@Thickness 3.20 mm
unannealed; ASTM D648
Vicat Softening Point 145 °CRate B/50; ASTM D1525
 145 °CRate B/120; ISO 306
 145 °CRate B/50; ISO 306
 205 °CRate A/50; ASTM D1525
 205 °CRate A/50; ISO 306
Flammability, UL94 HB
@Thickness 1.60 mm
UL 94 by SABIC-IP
Oxygen Index 21 %ISO 4589
Glow Wire Test 750 °C
@Thickness 1.00 mm
IEC 60695-2-12
 850 °C
@Thickness 3.00 mm
IEC 60695-2-12
 
Processing PropertiesOriginal ValueComments
Processing Temperature 40.0 - 60.0 °CHopper Temperature
Nozzle Temperature 240 - 260 °CInjection Molding
Zone 1 230 - 245 °C
Zone 2 240 - 255 °C
Zone 3 245 - 265 °C
Melt Temperature 250 - 270 °C
Mold Temperature 40.0 - 100 °C
Drying Temperature 110 - 120 °CInjection Molding
Dry Time 2.00 - 4.00 hourInjection Molding
Moisture Content 0.020 %

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PSABI10312 / 243779

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.