General Notes on Meldin 2000 Series Bearing Products: For High-Temperature, Close-Tolerance Applications. Able to withstand temperatures of 600°F with excursions to 900°F, the Medlin® 2000 Series can be machined into various configurations, from rod or sheet stock shapes. Black in color. Meldin® 2000 Series offers very high compression strength, high creep resistance, and dimensional stability. Specific Notes on Meldin® 2030 Bearing Meldin® 2030 bearing compound operates with extremely low friction in both dynamic and static applications, and provides thermal and electrical insulation.
Applications include: Appliances, Automotive, Industrial, Semiconductor, Transportation.
Specification Notes: Bushing Material Information provided by Saint Gobain Performance Products. |