Availability: North America Forms: Pellets Filler/Reinforcement: Glass Fiber Reinforcement, 13% Filler by Weight Additive: Heat Stabilizer and Impact Modifier Features: Heat Stabilized and Impact Modified Processing Method: Injection Molding Information provided by TP Composites, Inc. |