MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Rulon Bearings

(Viewing data as-entered. Click here to return)
Daikin DAI-EL® G-755BP Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content
Categories: Polymer; Thermoset; Fluoropolymer, TS; Thermoset Fluoroelastomer; Rubber or Thermoset Elastomer (TSE)

Material Notes: DAI-EL® G-755BP is a bisphenol curable, gum copolymer with medium Mooney viscosity. It is designed especially for extrusion and calendering.

Typical Applications: Hoses, thin sheets

Rheological Properties MDR 2000:
Temperature: 177°C
Frequency: 100 cpm
Strain: 0.5°
Test time: 6 min

Information provided by Daikin.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Specific Gravity 1.81 g/cc
Mooney Viscosity 29
@Temperature 121 °C
ML 1+10
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore A 73Press Cure: 10' @177°C/No postcure
 74Press Cure: 5' @177°C/Post Cure: 24 h @ 260°C
 75Press Cure: 10' @177°C/Post Cure: 24 h @ 232°C
Tensile Strength at Break 9.70 MPaPress Cure: 10' @177°C/No postcure
 13.1 MPaPress Cure: 5' @177°C/Post Cure: 24 h @ 260°C
 13.8 MPaPress Cure: 10' @177°C/Post Cure: 24 h @ 232°C
Elongation at Break 210 %Press Cure: 10' @177°C/Post Cure: 24 h @ 232°C
 210 %Press Cure: 5' @177°C/Post Cure: 24 h @ 260°C
 310 %Press Cure: 10' @177°C/No postcure
100% Modulus 3.70 MPa
@Strain 100 %
Press Cure: 10' @177°C/No postcure
 5.40 MPa
@Strain 100 %
Press Cure: 10' @177°C/Post Cure: 24 h @ 232°C
 5.70 MPa
@Strain 100 %
Press Cure: 5' @177°C/Post Cure: 24 h @ 260°C
Compression Set 15 %
@Temperature 200 °C,
Time 252000 sec
#214 O-ring, Press Cure: 10' @177°C/Post Cure: 24 h @ 232°C; ASTM D395 Method B
 20 %
@Temperature 200 °C,
Time 252000 sec
#214 O-ring, Press Cure: 5' @177°C/Post Cure: 24 h @ 260°C; ASTM D395 Method B
 49 %
@Temperature 200 °C,
Time 252000 sec
#214 O-ring, Press Cure: 10' @177°C/No postcure; ASTM D395 Method B
 
Thermal PropertiesOriginal ValueComments
Minimum Service Temperature, Air -18.0 °CLow Temperature Retraction; ASTM D1329
 
Processing PropertiesOriginal ValueComments
Cure Time 1.00 mints2, scorch time, MDR 2000
 1.20 mint'50, time to 50% cure, MDR 2000
 1.90 mint'90, time to 90% cure, MDR 2000
 10.0 min
@Temperature 177 °C
Press Cure, MDR 2000
 
Component Elements PropertiesOriginal ValueComments
Fluorine, F 66 %
 
Descriptive Properties
ColorWhite to pale brown
MH21.5 dNmmaximum torque, MDR 2000
ML1.2 dNmminimum torque, MDR 2000
Test Formula0.5 phrPhosphonium accelerator
 100 phrDAI-EL® G-755BP
 2 phrBisphenol AF
 3 phrMagnesium oxide
 30 phrMT Carbon Black (N-990)
 6 phrCalcium hydroxide

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Daikin DAI-EL® G-741-A Fluoroelastomer Copolymer, 66% Fluorine Content
Daikin DAI-EL® G-704BP Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content
Daikin DAI-EL® G-701HBP Fluoroelastomer Copolymer, Bisphenol Curable Grade, 66% Fluorine Content

PDAIJ9824 / 209895

Master Bond adhesives

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.