MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Scotchkote™ HG 519 Epoxy Ceramic HD Surfacer
Categories: Polymer; Thermoset; Epoxy

Material Notes: Scotchkote Epoxy Ceramic HD Surfacer HG 519 has been specifically developed as a 100% solids ceramic repair system for resurfacing equipment subject to severe abrasion.

Product Features:

  • Combines good application characteristics with excellent build capabilities.
  • Designed for application by trowel or spatula at thicknesses up to 12 mm
  • Provides outstanding resistance to sliding abrasion
  • Designed for use to rebuild worn hoppers, chutes, pipe elbows and other equipment subject to aggressive attack from dry solids and slurries
  • Excellent adhesion to correctly prepared metal surfaces

Information provided by 3M

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Solids Content 100 %
Thickness <= 6.00 mil
 
Mechanical PropertiesOriginal ValueComments
Hardness, Rockwell R 100ASTM D785
Flexural Strength 6000 psiASTM D790
Compressive Strength 15000 psiASTM D695
Shear Strength 2000 psiTensile Shear Adhesion, on a grit blasted steel; ASTM D1002
Abrasion 1.1[g] per 1000 cycles, 1 kg, CS17 Wheel; ASTM D4060
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 158 °CWet
 248 °CDry
Heat Distortion Temperature 60.0 °CASTM D648
 
Processing PropertiesOriginal ValueComments
Cure Time 8.00 hourHard Dry for machining
 120 hourFull Cure
 
Descriptive Properties
AppearanceGray

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PMM35293 / 170040

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.