Notes: Monprene CP-32054G CLR is a very soft clear low density thermoplastic elastomer gel designed for a variety of consumer product applications. Monprene CP-32054G CLR is a low density, high flow, high elasticity grade that is suitable for injection molding. Availability: Africa & Middle East; Europe; Asia Pacific; Latin America; North America Features: Contact Clarity; High Elasticity; High Flow; Low Density; Low Hardness; Low Specific Gravity; Without Fillers Uses: Consumer Applications; Footwear; Handles; Safety Equipment; Sporting Goods; Writing Instruments RoHS Compliance: RoHS Compliant Form: Pellets Processing Method: Injection Molding; Extrusion Information provided by Teknor Apex |