MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

(Viewing data as-entered. Click here to return)
Unifrax Fibermass® 2200 Ceramic Fiber Blocks
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Fibermass® ceramic fiber blocks combine advancements in fiber chemistry and manufacturing technology to provide an economical lining material for a wide range of heat processing equipment. The Fibermass manufacturing technique bonds layers of refractory ceramic fiber blanket into a strong, pliable fiber block. Spun ceramic fiber blankets which feature high tensile strength for improved resistance to mechanical abuse, vibration and gas velocity are used in the construction of Fibermass blocks. A proprietary fiber treatment decreases fiber dusting and irritation while increasing block flexibility, making the block easy to compress into place. Blocks are available in two temperature grades based on construction from Durablanket® HP-S or Durablanket 2600. The availability of standard or high-density blocks in each temperature grade results in a product which meets a wide range of application needs. Fibermass ceramic fiber block offer many of the same advantages as other Anchor-Loc® or Fiberwall® furnace linings when compared to refractory construction. They are:

  • Faster temperature cycling
  • Lower fuel costs
  • Lower installation cost
  • Resistance to thermal shock
  • Lower heat storage
  • Increased productivity
  • Easier repairs

  • Low mass kiln cars
  • Gas turbine exhaust ducts
  • Duct and stack linings
  • Regenerative thermal oxidizer
  • Furnace lining insulation for high-temperature applications
  • Roller hearth furnace linings
  • HRSG linings
  • Furnace hearths
  • Boiler insulation

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 8.00 lb/ft³Edge Grain
 10.0 lb/ft³Durablanket HP-S
 
Thermal PropertiesOriginal ValueComments
Maximum Service Temperature, Air 1149 °CRecommended Operating Temperature
 
Component Elements PropertiesOriginal ValueComments
Al2O3 43 - 47 %
NaO2 <= 0.50 %
SiO2 53 - 57 %
 
Descriptive Properties
Temperature Grade (°C)1260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unifrax Fiberfrax® Durablanket® 2600 Ceramic Fiber Insulator
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator
Unifrax Fiberfrax® Fibermat® Blanket Ceramic Fiber Insulator
Pyrotek Fiber Seal Y-1 Ceramic fiber paper
Unifrax Fiberfrax® Durablanket® HP-S Ceramic Fiber Insulator

CUNIF084 / 97856

Specialty Compounds RTP Company

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.