MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
BEWiSynbra Circulum® GF-514p Expandable Polystyrene
Categories: Polymer; Thermoplastic; Polystyrene (PS); Expanded Polystyrene (EPS)

Material Notes: Description: GF-514p is a flame retardant (FR) expandable polystyrene grade, containing graphite, with reduced thermal conductivity. Pentane is used as a blowing agent and a brominated polymeric flame retardant as an FR additive. The product is delivered in the form of spherical beads with a bulk density of about 0.6 g/cm3 and is available in 1100 kg octabins.

Applications: The properties of GF-514p make it suitable for the production of flame retardant light and heavy insulation board by block or shape moulding, in accordance with ISO EN 11925-2 class E.

Information provided by BEWi Synbra

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Bulk Density 0.600 g/cc
Storage Temperature 20.0 °C
 
Mechanical PropertiesOriginal ValueComments
Flexural Strength 0.130 MPa15 kg/m3; EN 12089
 0.200 MPa20 kg/m3; EN 12089
 0.260 MPa25 kg/m3; EN 12089
Compressive Strength 0.0700 MPa
@Strain 10 %
15 kg/m3; EN 826
 0.105 MPa
@Strain 10 %
20 kg/m3; EN 826
 0.140 MPa
@Strain 10 %
25 kg/m3; EN 826
 
Thermal PropertiesOriginal ValueComments
Thermal Conductivity 0.0290 W/m-K20 kg/m3; EN 12667
 0.0290 W/m-K25 kg/m3; EN 12667
 0.0310 W/m-K15 kg/m3; EN 12667
 
Descriptive Properties
Raw material<0.1%Monomer level
 0.8-1.6 mmMain bead size distribution
 5.5-6.5%Pentane content

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PBEWS037 / 250846

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.