MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
Unifrax Fiberfrax® Duraboard® 500ES Ceramic Fiber Board
Categories: Ceramic; Oxide; Aluminum Oxide; Silicon Oxide

Material Notes: Fiberfrax® Duraboard® products are a family of rigid, high-temperature ceramic fiber boards manufactured in a wet forming process using Fiberfrax alumina-silica fibers and binders. All Duraboard products offer low thermal conductivity, high temperature stability, uniform density, and excellent resistance to thermal shock and chemical attack.

This product uses a unique fiber formulation to obtain high strength and machinability not normally achieved in light-weight ceramic fiber board products. The innovative composite binder system using both inorganic and organic components results in a strength-to-weight ratio of more than three times that of standard refractory ceramic fiber boards. Improved physical characteristics of this product allows for easier handling and fabrication. Duraboard 500ES has more than four times the strength of standard boards of similar densities and thicknesses.

Description: Unique familiy of highly machinable lightweight boards manufactured with three to four times the green strength as standard board products.

Information Provided by Unifrax I LLC

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 22.0 lb/ft³Nominal
Loss On Ignition 4.0 - 8.0 %
 
Mechanical PropertiesOriginal ValueComments
Modulus of Rupture 0.170 ksiFired (24 hrs at cont. use)
 0.450 ksiGreen (typ.)
Compressive Strength 28.0 psi5% Deformation; Fired
 33.0 psi10% Deformation; Fired
 34.0 psi15% Deformation; Fired
 41.0 psi5% Deformation; Green
 65.0 psi10% Deformation; Green
 76.0 psi15% Deformation; Green
 
Electrical PropertiesOriginal ValueComments
Dielectric Strength 27.0 V/mil
 
Thermal PropertiesOriginal ValueComments
Melting Point 1760 °C
Maximum Service Temperature, Air 1149 °CRecommended Operating Temperature
Shrinkage <= 5.0 %
@Time 86400 sec
at Recommended Operating Temperature
 
Descriptive Properties
ColorCream to tan
Fiberfrax® Fibers (%)90
Temperature Grade (°C)1260

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Unifrax Fiberfrax® Durablanket® 2600 Ceramic Fiber Insulator
Unifrax Fiberfrax® Durablanket® S Ceramic Fiber Insulator
Unifrax Fiberfrax® Duraboard® 350ES Ceramic Fiber Board
Unifrax Fiberfrax® Fibermat® Blanket Ceramic Fiber Insulator
Unifrax Fiberfrax® Fibermax® Mat Ceramic Fiber Insulator

CUNIF030 / 97802

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.