MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

CRP  Windform

(Viewing data as-entered. Click here to return)
Carbon Printers RPU 70 Rigid Polyurethane
Categories: Polymer; 3D Printing/Additive Manufacturing Polymer; Thermoplastic; Polyurethane, TP

Material Notes: RPU 70 is a tough, heat resistant material that is a good choice for parts requiring strength, toughness, and moderate heat resistance.

Information provided by Carbon®

Vendors: Click here to view all available suppliers for this material.

Please click here if you are a supplier and would like information on how to add your listing to this material.

 
Physical PropertiesOriginal ValueComments
Density 1.01 g/ccliquid resin
 1.076 g/ccASTM D792
Water Absorption 1.01 %long term; ASTM D570
 0.31 %
@Time 86400 sec
ASTM D570
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 80ASTM D2240
Tensile Strength, Ultimate 43.0 - 47.0 MPaType V, 10 mm/min; ASTM D638
Tensile Strength, Yield 43.0 - 47.0 MPaType V, 10 mm/min; ASTM D638
Elongation at Break 80 - 120 %Type V, 10 mm/min; ASTM D638
Tensile Modulus 1700 - 2100 MPaType V, 10 mm/min; ASTM D638
Flexural Strength 53.0 - 71.0 MPaASTM D790
Flexural Modulus 1500 - 2100 MPaASTM D790
Izod Impact, Notched 15.0 - 23.0 J/m
@Temperature -30.0 °C
Machined; ASTM D256
 21.0 - 23.0 J/m
@Temperature 23.0 °C
Machined; ASTM D256
Izod Impact, Unnotched 500 - 560 J/mASTM D4812
Charpy Impact, Notched 1.68 - 1.98 kJ/m²ISO 179-1/1eA
Taber Abrasion, mg/1000 Cycles 70
@Load 1.00 kg
CS-17, 100 % vacuum; ASTM D4060
 
Thermal PropertiesOriginal ValueComments
CTE, linear 96.0 µm/m-°C
@Temperature -40.0 - 40.0 °C
ASTM E831
Deflection Temperature at 0.46 MPa (66 psi) 70.0 °CASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 55.0 °CASTM D648

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCARBP014 / 255846

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.