MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
Chevron Phillips Marlex® 4571 Polyethylene Film Grade LDPE
Categories: Polymer; Film; Thermoplastic; Polyethylene (PE); Low Density (LDPE); Low Density Polyethylene (LDPE), Film Grade

Material Notes: This low density polyethylene is tailored for cast film applications that require: • High speed extrusion • Low neck-in • Good drawdown • Edge tear resistance • High coefficient of friction

Typical cast film resin applications include: • Personal care • General purpose.

information provided by Chevron Phillips Chemical Company LP.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.924 g/ccASTM D1505
Water Vapor Transmission 13.0 g/m²/day
@Thickness 0.0317 mm
ASTM F1249
Oxygen Transmission Rate 6100 cc/m²/day
@Thickness 0.0317 mm
ASTM D3985
Thickness 1.25 milAs Tested
Melt Flow 4.1 g/10 min
@Load 2.16 kg,
Temperature 190 °C
ASTM D1238
Antiblock Level 0.000 ppm
Slip Level 0.000 ppm
 
Mechanical PropertiesOriginal ValueComments
Coefficient of Friction >= 0.75ASTM D1894
Elmendorf Tear Strength MD 320 g
@Thickness 0.0317 mm
ASTM D1922
Elmendorf Tear Strength TD 125 g
@Thickness 0.0317 mm
ASTM D1922
Elmendorf Tear Strength, MD 256 g/mil
@Thickness 0.0317 mm
ASTM D1922
Elmendorf Tear Strength, TD 100 g/mil
@Thickness 0.0317 mm
ASTM D1922
Dart Drop 52.0 g/mil
@Thickness 0.0317 mm
ASTM D1709
Dart Drop Test 65.0 g
@Thickness 0.0317 mm
ASTM D1709
 
Thermal PropertiesOriginal ValueComments
Melting Point 109 °CASTM D3418
Vicat Softening Point 99.0 °CASTM D1525
 
Optical PropertiesOriginal ValueComments
Haze 9.0 %
@Thickness 0.0317 mm
ASTM D1003
Gloss 86 %
@Thickness 0.0317 mm
60°; ASTM D2457

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

PCHEVC8903 / 241986

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.