MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Master Bond adhesives

(Viewing data as-entered. Click here to return)
3M Silux Plus™ Anterior Restorative Dental Composite
Categories: Polymer; Thermoset; Methacrylate

Material Notes: 3M Silux Plus™ anterior restorative provided superior esthetics that hold luster over time and a high degree of polishability to match enamel. It is available in multiple shade/opacity combinations to match surrounding teeth. It has a non-sticky, non-slumping consistency that adapts easily to margins, making it easy to place, mold, and sculpt. Bonding to tooth structure is accomplished by using a dental adhesive system, such as 3M™ Single Bond or 3M™ Scotchbond Multi-Purpose Adhesive Systems.

Silux Plus is silica filled (40% by volume) with an average particle size of 0.04 µm. Compared to other dental composites, it has a low diametral tensile strength, medium compressive strength, low-medium compressive modulus, low flexural strength and a low flexural modulus.

Information provided by 3M. Contact 3M for further information before specifying or using this product.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Processing PropertiesOriginal ValueComments
Processing Temperature 20.0 °CLight cured

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
AgPd-4 Precious dental alloy
HGC-1 Precious dental alloy
Kennametal Stellite Denertia™ C13 Cobalt Chromium Dental Alloy
Kennametal Stellite Denertia™ C14 Cobalt Chromium Dental Alloy
Kennametal Stellite Denertia™ C4 Cobalt Chromium Dental Alloy

PMMM03 / 53488

Rulon Bearings

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.