MatWeb - Material Property Data Advertise with MatWeb!     Register Now
Data sheets for over 180,000 metals, plastics, ceramics, and composites.
MatWeb - Material Property Data HOME  •   SEARCH  •   TOOLS  •   SUPPLIERS  •   FOLDERS  •   ABOUT US  •   FAQ  •   LOG IN    
Recently Viewed Materials (most recent at top)  

Login to see your most recently viewed materials here.

Or if you don't have an account with us yet, then click here to register.

  Searches:   Advanced  | Category  | Property  | Metals  | Trade Name  | Manufacturer  | Recently Viewed Materials
  

Elmet Technologies

(Viewing data as-entered. Click here to return)
UBE UMERIT 613A Metallocene LLDPE
Categories: Polymer; Thermoplastic; Polyethylene (PE); Linear Low Density (LLDPE); Linear Low Density Polyethylene (LLDPE), Injection Molded

Material Notes: Description: UBE Super Polyethylene Umerit® is an ethylene-olefin copolymer made by UBE using the metallocene catalytic method. The metallocene catalytic method results in superior physical properties by being able to acquire any targeted molecular structures. Specific Notes for this Grade: UMERIT® 613A offer various excellent properties: Superior transparency and low temperature flexibility, the surface of processed products is free from stickiness and cloud due to the elimination of low molecular weight elements, high reliability products are guaranteed due to superior mechanical properties, and high ESCR properties

Information provided by UBE.

Vendors: No vendors are listed for this material. Please click here if you are a supplier and would like information on how to add your listing to this material.
 
Physical PropertiesOriginal ValueComments
Density 0.913 g/ccASTM D1505
Environmental Stress Crack Resistance 20 hourF50; ASTM D1693
Melt Flow 30 g/10 minASTM D1238
 
Mechanical PropertiesOriginal ValueComments
Hardness, Shore D 50ASTM D2240
Tensile Strength, Yield 30.0 MPaASTM D638
Elongation at Break 850 %ASTM D638
Tensile Modulus 0.230 GPaBending Modulus; ASTM D790
 
Thermal PropertiesOriginal ValueComments
Melting Point 113 °CUBE method
Vicat Softening Point 87.0 °CASTM D1525

Some of the values displayed above may have been converted from their original units and/or rounded in order to display the information in a consistent format. Users requiring more precise data for scientific or engineering calculations can click on the property value to see the original value as well as raw conversions to equivalent units. We advise that you only use the original value or one of its raw conversions in your calculations to minimize rounding error. We also ask that you refer to MatWeb's terms of use regarding this information. Click here to go back to viewing the property data in MatWeb's normal format.

Users viewing this material also viewed the following:
Dow 959S Linear Low Density Polyethylene (LDPE)
Dow GRSN-9820 NT 7 Linear Low Density Polyethylene Granular Solid
Dow DNDA-8320 NT 7 Linear Low Density Polyethylene Resin
Dow DNDA-7340 NT 7 Linear Low Density Polyethylene Resin
Dow DNDA-7144 NT 7 Linear Low Density Polyethylene Resin

PUBE006 / 71566

Ensinger PEI

Please read our License Agreement regarding materials data and our Privacy Policy. Questions or comments about MatWeb? Please contact us at webmaster@matweb.com. We appreciate your input.

The contents of this web site, the MatWeb logo, and "MatWeb" are Copyright 1996-2024 by MatWeb, LLC. MatWeb is intended for personal, non-commercial use. The contents, results, and technical data from this site may not be reproduced either electronically, photographically or substantively without permission from MatWeb, LLC.